ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

FRP Ladder & Stair Systems

Non-conductive · slip resistant · OSHA compliant

FRP Ladder & Stair Systems
Product Overview

FRP Ladder & Stair Systems

From vertical ladders with safety cages to stair treads and complete stair systems, ZeAllgrate manufactures FRP access systems that protect workers in wet, corrosive and electrically sensitive environments.

  • Vertical & fixed ladders with safety cage options
  • Non-conductive — safe for electrical work zones
  • Slip-resistant rungs and stair treads
  • OSHA & ISO compliance
  • Complete bolt-together systems — no welding
  • Stair treads in molded or pultruded grating
Key Specifications

Technical Data

Ladder TypeVertical / Inclined / Cage
Rung Spacing250 / 300 mm
Stair Angle30° – 45°
TreadMolded / Pultruded FRP grating
CageFRP hoop & vertical bars
HardwareSS304 / SS316
Load150 kg concentrated rung load
FinishGrit-top anti-slip standard
Engineering Drawings

Product Drawings & Details

Dimensioned drawings for specification and fabrication — matching the technical documentation of leading FRP manufacturers.

DW-01 Elevation — Complete Handrail Assembly
DWG NO: ZL-HDG-01SCALE 1:10UNITS: mmMAT: FRPTop rail 40×40Mid railKickplate 3 mmPost1100 mm1200 mmISO 14122-3 1100 mm / OSHA 42 in — 890 N load test
DW-02 Post Base — Floor Mounting Detail
DWG NO: ZL-HDG-02SCALE 1:10UNITS: mmMAT: FRPPostBase plate 150×150×8Concrete floorM12 anchorM12150×150
DW-03 Post-to-Rail Connection Node
DWG NO: ZL-HDG-03SCALE 1:10UNITS: mmMAT: FRPTop railPostGusset angleM8 boltsAll fasteners SS304; torque per spec sheet
DW-04 Stair Handrail — Rake Profile
DWG NO: ZL-HDG-04SCALE 1:10UNITS: mmMAT: FRPRake railKickplate30–38° rake per OSHA/ISOH
Standard Configurations

Full Specification Matrix

Standard stocked configurations covering mesh, thickness, panel sizes and unit weights. Custom configurations available on request.

ParameterStandardOptions
Ladder TypeVertical / InclinedCage: hoops + vertical bars
Rung Spacing250 / 300 mmCustom per code
Rung Diameter25 / 32 mmGrit-top anti-slip standard
Stair Angle30° – 45°Per site layout
TreadMolded / Pultruded gratingGrit-top standard
Rung Load150 kg concentratedHigher ratings on request

Values are standard industry configurations. Certified load/span charts and test reports provided with every order.

Material Properties

Physical & Mechanical Properties

Typical values tested in accordance with ASTM methods on production panels. Certified test reports available on request.

PropertyValueTest Method
Tensile Strength (longitudinal)220 MPaASTM D638
Flexural Strength240 MPaASTM D790
Compressive Strength240 MPaASTM D695
Flexural Modulus13 GPaASTM D790
Density1.9 g/cm³ASTM D792
Water Absorption (24h)< 0.3%ASTM D570
Barcol Hardness50 – 60ASTM D2583
Flame Spread≤ 25 (Class A)ASTM E84
Product Gallery

In Production & In the Field

Real photographs from our manufacturing facility and installed projects.

Standards & Compliance

Engineered to International Standards

A

ASTM E84

Surface burning characteristics for fire-retardant grades — Class A/Class B options.

I

ISO 14122

Permanent means of access to machinery — platform, walkway and stair requirements.

S

AS 1657

Fixed platforms, walkways, stairways and ladders — design, construction and testing.

O

OSHA 1910

Walking-working surfaces and fall protection compliance for industrial installations.

Material certificates, load test reports and compliance documentation shipped with every order. Certified: ISO 9001:2015 · DNV & ABS Marine · SGS & Intertek. View certifications →

Surfaces & Colors

Options for Every Environment

SurfaceBest ForAnti-Slip
Concave / ConvexGeneral industrial walkways, platformsStandard molded profile
Grit-Top (Silica)Wet, oily and chemical process areasHigh — embedded silica grit
Micro-MeshPublic access, ADA-compliant small openingsHigh — small mesh profile
MeniscusLight pedestrian traffic, aestheticsModerate — meniscus surface

Standard colors: Green (RAL 6010), Gray (RAL 7047), Yellow (RAL 1003), Red, Blue, Black — custom Pantone/RAL matching available.

Chemical Resistance

Chemical Resistance Reference

Indicative chemical resistance by resin system — the basis of every material selection. Always confirm the final recommendation against our certified chemical resistance guide for your specific media, concentration and temperature.

Chemical MediumISO PolyesterVinyl EsterPhenolicService Notes
Sulfuric AcidGoodExcellentFairUp to 50%, 50 °C
Hydrochloric AcidGoodExcellentPoorUp to 37%, 50 °C
Sodium Hydroxide (Caustic)GoodGoodFairUp to 25%, 50 °C
Sodium Hypochlorite (Bleach)FairExcellentPoorUp to 15%, 40 °C
Hydrogen PeroxideFairGoodFairUp to 30%, 40 °C
Organic SolventsFairGoodPoorModerate temperature
Seawater / Salt SprayExcellentExcellentExcellentContinuous marine service
Petroleum / HydrocarbonsGoodExcellentFairModerate temperature
Acetic AcidGoodExcellentFairUp to 25%, 50 °C
Phosphoric AcidGoodExcellentFairUp to 85%, 60 °C

Ratings: Excellent — long-term service; Good — suitable with normal inspection; Fair — limited service, verify application. Full Chemical Resistance Guide →

Resin Systems

Ten Resin Systems for Every Chemical Environment

Corrosion resistance starts with the resin. ZeAllgrate manufactures in ten engineered resin systems, matching the industry’s proven material selection methodology.

Resin SystemKey PropertyMax Service TempTypical Use
Isophthalic Polyester (ISO)General corrosion resistance60 – 70 °CWater/wastewater, industrial floors
ISO Chemical GradeEnhanced chemical resistance70 – 80 °CChemical plant walkways
Vinyl Ester (VE)Superior acid/alkali/solvent resistance80 – 90 °CChemical, bleaching, pulp
VE Chemical GradeMaximum corrosion performance90 – 100 °CHarshest chemical exposure
PhenolicLow smoke, low flame spread120 – 150 °COffshore, fire-critical
Fire Retardant (FR)ASTM E84 Class A, flame spread ≤ 2560 – 70 °CCode-required flame ratings
UV-StabilizedOutdoor UV resistance60 – 70 °CSolar-exposed installations
Heat ResistantHigh-temperature service100 – 120 °CProcess heat areas
Conductive (Carbon)Static-dissipative60 – 70 °CElectrical / explosion areas
Food Grade (FDA)FDA-compliant contact surfaces60 – 70 °CFood & beverage processing

Our engineers prepare a written resin recommendation with every quotation — matched to your media, concentration and service temperature.

Installation

Installation Notes

✂

Cutting

Carbide-tipped or abrasive cutters; support both sides of the cut; wear dust protection. Wet cutting recommended.

🔩

Fastening

Fasten every panel at every support intersection. SS304/316 G-clips in corrosive service; expansion bolts for concrete.

↔

Orientation

Pultruded bearing bars run across the span — never parallel. Leave thermal gaps at fixed supports.

Installation ParameterRecommended PracticeStandard Reference
Support SpacingMaximum span per certified load chart — never exceed recommended clear spanLoad chart per configuration
BearingMinimum 40 mm bearing on each supportZeAllgrate practice / ISO 14122-3
Fastener SpacingMinimum 2 hold-down clips per support beam, spaced ≤ 1219 mm (4 ft) on centre; minimum 4 clips per panelPer ZeAllgrate engineering practice
Thermal ExpansionAllow 3 – 5 mm expansion gap at fixed supports; molded coefficient ≈ 15–25×10⁻⁶ /°C (direction dependent)Manufacturer data
Cut HolesSeal cut edges in chemical service with resin; radius corners to avoid stress pointsDesign guide
Fall ProtectionHandrail height ≥ 1100 mm (ISO 14122-3) / 42 in (OSHA 1910.23); kickplate where requiredOSHA 1910 / ISO 14122

Full Installation Guide →

Resin Systems

Choose the Right Resin for Your Environment

Corrosion resistance starts with the resin system. ZeAllgrate offers 3+ engineered resin systems for every chemical environment.

Isophthalic PolyesterGeneral-purpose corrosion resistance; excellent value for industrial and water/wastewater applications
Vinyl EsterSuperior chemical resistance to acids, alkalis and solvents — for chemical plants and bleaching environments
PhenolicLow smoke, low flame spread and high-temperature performance — for fire-critical and offshore applications
Fire-Retardant (FR)Enhanced flame-retardant grades meeting surface-burning requirements (ASTM E84)
UV-StabilizedUV-inhibited formulations for outdoor and solar-exposed installations

Contact our engineers for a chemical-resistance recommendation matched to your specific media, concentration and temperature.

Selection Process

How to Specify in Four Steps

1

Define Environment

Identify chemicals, temperature, UV exposure and load requirements.

2

Choose Grating Type

Molded for bi-directional strength; pultruded for long spans and heavy loads.

3

Check Load / Span

Verify the support span against certified load charts for your configuration.

4

Specify Surface & Clips

Grit-top for wet areas; SS304/316 clips for secure fastening.

Full Design Guide →

Technical Documents

Datasheets & Downloads

FRP Ladder & Stair Systems - Technical Data Sheet
PDF · Technical Document
Download
ZeAllgrate Product Catalog
PDF · Technical Document
Download
FRP Grating Design Guide
PDF · Technical Document
Download
FAQ

Frequently Asked Questions

What is the lead time?

Standard panels: 7-15 days production; custom fabrication 15-20 days, plus shipping time. Urgent orders can be prioritized.

Can I get a free sample?

Yes - free small samples are available for evaluation. Contact sales@izeall.com with your application details.

What certificates do you provide?

Material certificates and load test reports are supplied with every shipment. Our facility is ISO 9001:2015 certified; marine grades carry DNV & ABS approvals, and third-party SGS & Intertek inspection and testing is available on request.

Related Technical Articles

Go Deeper with the ZeAllgrate Knowledge Base

📚

Stair Tread Installation

Panel sizing, nosing and fixing for FRP stair treads.

Read article →
📚

ISO 14122 & AS 1657

International access-system standards for ladders and stairs.

Read article →
📚

Installation Tolerances

Fit-up, leveling and field adjustment allowances.

Read article →

Need Safety Access Systems?

Send us your dimensions and environment — we'll confirm availability and pricing within 24 hours.