ZeAllgrate FRP Molded Grating
Our molded FRP grating (also known as molded GRP grating or fiberglass molded grating) is compression-molded from continuous glass fiber rovings and thermoset resin, delivering uniform bi-directional strength ideal for walkways, platforms, and trench covers.

ZeAllgrate FRP Molded Grating
As a leading fiberglass grating manufacturer and FRP grating supplier, ZeAllgrate molded grating is manufactured in a compression molding process that interlocks continuous glass fibers in two directions — also known as GRP grating, GFRP grating, composite grating, fiberglass reinforced plastic grating or glass reinforced plastic grating — delivering exceptional bi-directional strength and impact resistance. It is the world's most widely specified FRP grate, GRP grate and composite grating — and ours is engineered for the harshest service conditions. If you prefer British English, the same panels are also listed as moulded GRP grating across our UK and Commonwealth documentation.
- Bi-directional strength: equal load capacity in both panel directions
- Anti-slip surfaces: concave/convex, grit-top (silica) options
- 3+ resin systems: isophthalic, vinyl ester, phenolic, fire-retardant
- FRP grating panel (GRP grating panel, fiberglass grating panel) sizes up to 1220 × 3660 mm; thickness 25 / 30 / 38 / 40 / 50 mm
- Non-conductive, non-magnetic, spark-resistant
- Service life 20+ years with zero maintenance in corrosive service
Technical Data
| Standard FRP grating panel | 1220 × 3660 mm (4' × 12') |
| Thickness | 25 / 30 / 38 / 40 / 50 mm |
| Mesh Pitch | 38×38 / 40×40 / 50×50 mm |
| Glass Content | 33% ± 3% (molded) |
| Surface | Concave / Convex / Grit-top |
| Resin Systems | ISO Polyester / Vinyl Ester / Phenolic / Fire-Retardant |
| Colors | Green, Gray, Yellow, Red, Blue, Custom |
| Load Test | Per ASTM E84, ISO 14122 |
Product Drawings & Details
Dimensioned drawings for specification and fabrication — matching the technical documentation of leading FRP manufacturers.
Full Specification Matrix
Standard stocked configurations covering mesh, thickness, FRP grating panel, GRP grating panel and fiberglass grating panel sizes and unit weights. Custom configurations available on request.
| Thickness | Mesh Pattern | FRP grating panel Sizes (m) | Open Area | Weight (kg/m²) |
|---|---|---|---|---|
| 25.4 mm | 38.1 × 38.1 mm square | 0.91 × 3.05 / 1.22 × 3.66 | 70% | 12.7 |
| 25.4 mm | 25.4 × 101.6 mm rectangular | 0.91 × 3.05 / 1.22 × 3.66 | 69% | 13.7 |
| 38.1 mm | 38.1 × 38.1 mm square | 0.91 × 3.05 / 1.52 × 3.05 / 1.22 × 3.66 / 1.52 × 3.66 | 70% | 18.6 |
| 38.1 mm | Mini-Mesh 19.05 × 19.05 top, 38.1 × 38.1 bottom | 1.22 × 3.66 | 44% | 22.0 |
| 50.8 mm | 50.8 × 50.8 mm square | 1.22 × 3.66 | 72% | 19.5 |
| 25.4 mm | Micro-Mesh 19.05 × 19.05 top, 38.1 × 38.1 bottom | 1.22 × 3.66 | 44% | 14.2 |
| 38.1 mm | HLC 25.4 × 50.8 mm rectangular | 1.22 × 3.66 | 48% | 30.3 |
| 50.8 mm | HLC 25.4 × 50.8 mm rectangular | 1.22 × 3.66 | 48% | 41.0 |
Values are standard industry configurations. Certified load/span charts and test reports provided with every order.
Load & Span Reference Table
Indicative allowable loads by span. Verify final design against certified load charts for your exact configuration.
| Span | CL 25 mm | CL 38 mm | CL 50 mm | UDL 25 mm | UDL 38 mm | UDL 50 mm |
|---|---|---|---|---|---|---|
| 460 mm | 412 kgf | 564 kgf | 1,161 kgf | 2,600 kgf/m² | 3,400 kgf/m² | 5,200 kgf/m² |
| 610 mm | 240 kgf | 377 kgf | 732 kgf | 1,900 kgf/m² | 2,500 kgf/m² | 3,800 kgf/m² |
| 915 mm | 120 kgf | 167 kgf | 341 kgf | 900 kgf/m² | 1,200 kgf/m² | 1,900 kgf/m² |
| 1220 mm | 60 kgf | 92 kgf | 197 kgf | 480 kgf/m² | 640 kgf/m² | 1,000 kgf/m² |
Molded GRP Grating — Load Capacity Table
Detailed allowable point load (kN), uniformly distributed load (kN/m²) and deflection (mm) by span and mesh configuration.
Note: All values are for standard isophthalic polyester resin at 25°C. Actual load capacity depends on resin type, panel orientation, and installation method. Contact our engineering team for load calculations for your specific application.
Table 1 — 38 mm Molded Grid (38×38 mm mesh)
| Span (mm) | Point Load (kN) | Distributed Load (kN/m²) | Deflection (mm) |
|---|---|---|---|
| 400 | 5.0 | 12.5 | 1.5 |
| 600 | 3.0 | 7.5 | 2.8 |
| 800 | 1.8 | 4.5 | 4.5 |
| 1000 | 1.2 | 3.0 | 6.8 |
| 1200 | 0.8 | 2.0 | 9.5 |
| 1400 | 0.6 | 1.5 | 12.8 |
Table 2 — 38 mm Mini Mesh (19×19 mm mesh)
| Span (mm) | Point Load (kN) | Distributed Load (kN/m²) |
|---|---|---|
| 400 | 6.5 | 16.0 |
| 600 | 4.0 | 10.0 |
| 800 | 2.5 | 6.0 |
| 1000 | 1.6 | 4.0 |
Table 3 — 50 mm Heavy Duty (50×50 mm mesh)
| Span (mm) | Point Load (kN) | Distributed Load (kN/m²) |
|---|---|---|
| 600 | 8.0 | 20.0 |
| 800 | 5.0 | 12.5 |
| 1000 | 3.2 | 8.0 |
| 1200 | 2.2 | 5.5 |
| 1400 | 1.6 | 4.0 |
| 1600 | 1.2 | 3.0 |
Find your clear span (the distance between two supports) in the left column, then read across to the point load (kN) and uniformly distributed load (kN/m²) for your panel thickness and mesh. The deflection column shows expected mid-span deflection under that load. Always design to a working load with a safety factor of at least 3 against ultimate failure, and keep deflection within the project limit (typically L/150 for walkways, L/200 for platforms).
Point load (concentrated load, kN) simulates a wheel, drum, valve operator or foot traffic applied over a small area — used for forklift, pallet-jack and drop-load checks. Uniformly distributed load (UDL, kN/m²) covers the whole panel area with even weight — used for pedestrian crowds, equipment weight and live loads on walkways. A panel must pass both checks; point load often governs on shorter spans while UDL governs on longer spans.
Not dramatically — the stiffness (modulus) and strength of the glass fibers dominate load capacity, and resin type affects corrosion and temperature resistance more than raw bending strength. However, vinyl ester panels retain their rated load better at elevated temperatures (HDT 120–150°C vs. 70–85°C for isophthalic) and after long-term chemical exposure, so in hot or corrosive service the de-rated working load is meaningfully higher than isophthalic. Ask engineering for a de-rated chart for your exact media and temperature.
Physical & Mechanical Properties
Typical values tested in accordance with ASTM methods on production FRP grating panels (GRP grating panels, fiberglass grating panels). Certified test reports available on request.
| Property | Value | Test Method |
|---|---|---|
| Tensile Strength | 70 MPa | ASTM D638 |
| Flexural Strength | 110 MPa | ASTM D790 |
| Compressive Strength | 170 MPa | ASTM D695 |
| Flexural Modulus | 8 GPa | ASTM D790 |
| Density | 1.7 g/cm³ | ASTM D792 |
| Water Absorption (24h) | < 0.5% | ASTM D570 |
| Barcol Hardness | 40 – 50 | ASTM D2583 |
| Flame Spread | ≤ 25 (Class A) | ASTM E84 |
Section Properties per Unit Width
Area (A), moment of inertia (I) and section modulus (S) per metre of panel width — for structural design of platforms and walkways.
| Configuration | Depth | Mesh | A (mm²/m) | I (×10⁶ mm⁴/m) | S (×10³ mm³/m) |
|---|---|---|---|---|---|
| Std 25.4 | 25.4 mm | 38.1 × 38.1 sq | 3.62 × 10³ | 0.191 | 15.6 |
| Std 25.4 R | 25.4 mm | 25.4 × 101.6 rect | 5.44 × 10³ | 0.300 | 23.1 |
| Std 38.1 | 38.1 mm | 38.1 × 38.1 sq | 6.03 × 10³ | 0.696 | 34.9 |
| Mini-Mesh 38.1 | 38.1 mm | 19.05 / 38.1 | 7.98 × 10³ | 0.975 | 42.6 |
| Std 50.8 | 50.8 mm | 50.8 × 50.8 sq | 6.09 × 10³ | 1.311 | 50.5 |
Indicative design values. Structural design should be verified by a qualified engineer against certified section data for the exact resin and configuration.
In Production & In the Field
Real photographs from our manufacturing facility and installed projects.
See How ZeAllgrate Is Made
Compression molding & pultrusion lines at our facility — ISO 9001:2015 certified.
Engineered to International Standards
ASTM E84
Surface burning characteristics for fire-retardant grades — Class A/Class B options.
ISO 14122
Permanent means of access to machinery — platform, walkway and stair requirements.
AS 1657
Fixed platforms, walkways, stairways and ladders — design, construction and testing.
OSHA 1910
Walking-working surfaces and fall protection compliance for industrial installations.
Material certificates, load test reports and compliance documentation shipped with every order. Certified: ISO 9001:2015 · DNV & ABS Marine · SGS & Intertek. View certifications →
Options for Every Environment
| Surface | Best For | Anti-Slip |
|---|---|---|
| Concave / Convex | General industrial walkways, platforms | Standard molded profile |
| Grit-Top (Silica) | Wet, oily and chemical process areas | High — embedded silica grit |
| Micro-Mesh | Public access, ADA-compliant small openings | High — small mesh profile |
| Meniscus | Light pedestrian traffic, aesthetics | Moderate — meniscus surface |
Standard colors: Green (RAL 6010), Gray (RAL 7047), Yellow (RAL 1003), Red, Blue, Black — custom Pantone/RAL matching available.
Chemical Resistance Reference
Indicative chemical resistance by resin system — the basis of every material selection. Always confirm the final recommendation against our certified chemical resistance guide for your specific media, concentration and temperature.
| Chemical Medium | ISO Polyester | Vinyl Ester | Phenolic | Service Notes |
|---|---|---|---|---|
| Sulfuric Acid | Good | Excellent | Fair | Up to 50%, 50 °C |
| Hydrochloric Acid | Good | Excellent | Poor | Up to 37%, 50 °C |
| Sodium Hydroxide (Caustic) | Good | Good | Fair | Up to 25%, 50 °C |
| Sodium Hypochlorite (Bleach) | Fair | Excellent | Poor | Up to 15%, 40 °C |
| Hydrogen Peroxide | Fair | Good | Fair | Up to 30%, 40 °C |
| Organic Solvents | Fair | Good | Poor | Moderate temperature |
| Seawater / Salt Spray | Excellent | Excellent | Excellent | Continuous marine service |
| Petroleum / Hydrocarbons | Good | Excellent | Fair | Moderate temperature |
| Acetic Acid | Good | Excellent | Fair | Up to 25%, 50 °C |
| Phosphoric Acid | Good | Excellent | Fair | Up to 85%, 60 °C |
Ratings: Excellent — long-term service; Good — suitable with normal inspection; Fair — limited service, verify application. Full Chemical Resistance Guide →
Ten Resin Systems for Every Chemical Environment
Corrosion resistance starts with the resin. ZeAllgrate manufactures in ten engineered resin systems, matching the industry’s proven material selection methodology.
| Resin System | Key Property | Max Service Temp | Typical Use |
|---|---|---|---|
| Isophthalic Polyester (ISO) | General corrosion resistance | 60 – 70 °C | Water/wastewater, industrial floors |
| ISO Chemical Grade | Enhanced chemical resistance | 70 – 80 °C | Chemical plant walkways |
| Vinyl Ester (VE) | Superior acid/alkali/solvent resistance | 80 – 90 °C | Chemical, bleaching, pulp |
| VE Chemical Grade | Maximum corrosion performance | 90 – 100 °C | Harshest chemical exposure |
| Phenolic | Low smoke, low flame spread | 120 – 150 °C | Offshore, fire-critical |
| Fire Retardant (FR) | ASTM E84 Class B, flame spread ≤ 25 | 60 – 70 °C | Code-required flame ratings |
| UV-Stabilized | Outdoor UV resistance | 60 – 70 °C | Solar-exposed installations |
| Heat Resistant | High-temperature service | 100 – 120 °C | Process heat areas |
| Conductive (Carbon) | Static-dissipative | 60 – 70 °C | Electrical / explosion areas |
| Food Grade (FDA) | FDA-compliant contact surfaces | 60 – 70 °C | Food & beverage processing |
Our engineers prepare a written resin recommendation with every quotation — matched to your media, concentration and service temperature.
Installation Notes
Cutting
Carbide-tipped or abrasive cutters; support both sides of the cut; wear dust protection. Wet cutting recommended.
Fastening
Fasten every FRP grating panel (GRP grating panel, fiberglass grating panel) at every support intersection. SS304/316 G-clips in corrosive service; expansion bolts for concrete.
Orientation
Pultruded bearing bars run across the span — never parallel. Leave thermal gaps at fixed supports.
| Installation Parameter | Recommended Practice | Standard Reference |
|---|---|---|
| Support Spacing | Maximum span per certified load chart — never exceed recommended clear span | Load chart per configuration |
| Bearing | Minimum 40 mm bearing on each support | ZeAllgrate practice / ISO 14122-3 |
| Fastener Spacing | Minimum 2 hold-down clips per support beam, spaced ≤ 1219 mm (4 ft) on centre; minimum 4 clips per FRP grating panel / GRP grating panel / fiberglass grating panel | Per ZeAllgrate engineering practice |
| Thermal Expansion | Allow 3 – 5 mm expansion gap at fixed supports; molded coefficient ≈ 15–25×10⁻⁶ /°C (direction dependent) | Manufacturer data |
| Cut Holes | Seal cut edges in chemical service with resin; radius corners to avoid stress points | Design guide |
| Fall Protection | Handrail height ≥ 1100 mm (ISO 14122-3) / 42 in (OSHA 1910.23); kickplate where required | OSHA 1910 / ISO 14122 |
Installed Projects
Real installations of ZeAllgrate products across industries.
Choose the Right Resin for Your Environment
Corrosion resistance starts with the resin system. ZeAllgrate offers 3+ engineered resin systems for every chemical environment.
| Isophthalic Polyester | General-purpose corrosion resistance; excellent value for industrial and water/wastewater applications |
| Vinyl Ester | Superior chemical resistance to acids, alkalis and solvents — for chemical plants and bleaching environments |
| Phenolic | Low smoke, low flame spread and high-temperature performance — for fire-critical and offshore applications |
| Fire-Retardant (FR) | Enhanced flame-retardant grades meeting surface-burning requirements (ASTM E84) |
| UV-Stabilized | UV-inhibited formulations for outdoor and solar-exposed installations |
Contact our engineers for a chemical-resistance recommendation matched to your specific media, concentration and temperature.
How to Specify in Four Steps
Define Environment
Identify chemicals, temperature, UV exposure and load requirements.
Choose Grating Type
Molded for bi-directional strength; pultruded for long spans and heavy loads.
Check Load / Span
Verify the support span against certified load charts for your configuration.
Specify Surface & Clips
Grit-top for wet areas; SS304/316 clips for secure fastening.
Frequently Asked Questions
Standard panels: 7-15 days production; custom fabrication 15-20 days, plus shipping time. Urgent orders can be prioritized.
Yes - free small samples are available for evaluation. Contact sales@izeall.com with your application details.
Material certificates and load test reports are supplied with every shipment. Our facility is ISO 9001:2015 certified; marine grades carry DNV & ABS approvals, and third-party SGS & Intertek inspection and testing is available on request.
GRP Grating Subcategories from Molded Panels
Specialized molded GRP grating variants — all produced on the same line as our standard molded panels.
Explore FRP Grating Types
Choose the right fiberglass grating, GRP grating and composite grating for your project — molded, pultruded, grille and clip systems.
FRP Grating
View →Molded & pultruded FRP grating panels, FRP grate and composite grating for walkways, platforms and trench covers.
GRP Grating
View →Glass reinforced plastic grating panels, GRP grate and GFRP grating from a certified GRP grating factory.
Fiberglass Grating
View →Fiberglass grating panels, fiberglass grate and fibreglass grating for industrial flooring and walkways.
FRP Grille
View →Fiberglass grille, tree grate, tree pit grating and architectural FRP grate.
Pultruded FRP Grating
View →Pultruded fiberglass grating, pultruded GRP grating and FRP pultruded bar grating for long spans.
Grating Clips & Clamps
View →FRP grating clips, clamps and fasteners in SS304/SS316 and galvanized steel.
Go Deeper with the ZeAllgrate Knowledge Base
Molded vs. Pultruded Grating
Read article →When to choose bi-directional molded or unidirectional pultruded strength.
Load & Deflection Selection
Read article →Match load class and span to panel stiffness and deflection limits.
Anti-Slip Surfaces Compared
Read article →Grit-top, concave and silica-cast surfaces and their slip ratings.
Installation Tips
Read article →Clips, cutting, expansion gaps and common field mistakes.
Chemical Resistance & Resin Selection
Read article →Corrosion performance of each resin system against aggressive media.
Load & Span Tables
Read article →Certified load classes and maximum clear spans by configuration.
What We Supply & Where It Goes
As an established FRP grating manufacturer, fiberglass grating supplier and GRP grating factory, ZeAllgrate supplies molded FRP grating, moulded GRP grating (British spelling), molded fiberglass grating, FRP molded grating and mini mesh FRP grating — in covered, gritted, concave surface, fiberglass phenolic and iso resin grades. We deliver custom FRP grating and cut to size FRP grating for export worldwide. For longer spans, pair with our pultruded FRP grating and FRP pultruded bar grating.
Applications
- FRP walkway grating & fiberglass platform grating
- FRP trench cover grating & FRP drainage grating
- Car wash FRP grating & solar rooftop FRP walkway grating
- FRP stair tread grating & dock fiberglass deck grating
- Offshore FRP grating & wastewater treatment FRP grating
- Chemical plant FRP platform grating
- FRP tree grate / FRP tree pit grating
- Livestock fiberglass flooring grating & pigeon floor FRP grating
- Swimming pool overflow FRP grating
Properties & Panel Formats
- Anti-slip FRP grating & corrosion resistant fiberglass grating
- Heavy duty GRP grating, lightweight FRP grating & high strength composite grating
- Non conductive FRP grating, fire retardant fiberglass grating & UV resistant GRP grating
- Industrial fiberglass flooring grating & fiberglass floor grating panel
- FRP grid panel, fiberglass mesh grating & FRP flooring sheet
- Concave surface FRP grating, gritted FRP grating & FRP covered grating
- Micro mesh fiberglass grating, fiberglass phenolic grating & iso resin FRP grating
Need a specific FRP grating panel size, mesh or resin? Tell us your span, load and environment — we cut to size and fabricate to your drawing. We can also tailor resin, mesh and finish to suit any moulded specification you provide.
Heavy-Duty Molded Grating
Heavy-duty molded grating is built for platforms, truck-bypass areas and equipment zones where dropped loads and occasional wheeling must not damage the bi-directional mesh. Higher glass content and thicker bars deliver the required point-load rating while keeping the panel field-cuttable.
Lightweight FRP Grating Panels
Lightweight FRP grating panels (about 13–20 kg/m² depending on thickness) hand-lay without lifting equipment, lowering rigging and labour on retrofits and rooftop works. Despite the low weight, molded panels retain enough stiffness for standard pedestrian and light-vehicle access.
Key Technical Specifications
| Parameter | Value |
|---|---|
| Temperature Range | -40°C to 120°C continuous (vinyl ester resin) |
| Load Capacity | Up to 100 kN/m² (forklift rated, heavy duty) |
| Maximum Span | Up to 3.6 meters (pultruded I-bar long span) |
| Standard Panel Size | 1220 × 3660 mm (molded standard) |
| Design Life | 25+ years in corrosive service |
| Weight vs Steel | 75% lighter than equivalent steel grating |
| Fire Rating | ASTM E84 Class B (flame spread ≤ 25, smoke developed ≤ 450; phenolic resin option) |
| Compliance | Compliant with BS EN 13700 (molded grating); ASTM E84 Class B |
| Resin Options | Isophthalic, Vinyl Ester, Phenolic, Food-Grade NSF |
When to Choose FRP vs Steel Grating
If your walkway is indoors, dry, and never sees a chemical spill, hot-dip galvanized steel grating may be cheaper. FRP earns its cost where steel becomes a maintenance item: acid spills, chlorides, salt air, wash-down areas, and corrosive environments. We'll tell you honestly if steel is the better choice for your project.
Installation Do's & Don'ts
✅ Do's
- Seal every cut edge with resin — unsealed edges wick moisture and degrade from the cut inward
- Use hold-down clips designed for grating — they don't damage the bearing bars
- Support panels at the recommended span — over-spanning causes deflection and premature failure
- Wear safety gear when cutting — fiberglass dust irritates skin and lungs
❌ Don'ts
- Do not drill through bearing bars to bolt it down — this removes exactly the material carrying the load
- Do not weld near installed grating — FRP is not steel, hot work damages panels and releases fumes
- Do not leave cut edges unsealed — this is the #1 reason FRP grating fails prematurely in service
- Do not mix hardware alloys on one deck — stainless steel 304 in chloride service will corrode
What to Send When Requesting a Quote
- Environment — Which chemicals are present? What concentrations? Are spills occasional or continuous?
- Load — Pedestrian only? Hand carts? Forklift traffic? Any point loads?
- Span — What is the clear distance between supports?
- Area & Layout — Total square meters? Any cut-outs, pipe penetrations, or irregular shapes?
- Surface — Smooth top? Gritted anti-slip? Mini-mesh for foot traffic?
- Fire Requirements — Is flame-retardant resin required? What flame-spread rating?
- Color — Any color preference for safety marking or plant convention?
Where This Grating Is Specified
Explore the application pages that use this molded FRP / GRP grating — each with load classes, resin recommendations and reference projects.
Engineering Articles & Buying Guides
Deep technical resources to help you specify, install and maintain FRP / GRP grating correctly.
What Is FRP Grating?
Complete guide to fiberglass reinforced plastic grating — how it's made, molded vs pultruded, properties and applications vs steel.
FRP vs Steel Grating Lifecycle Cost
Total cost of ownership comparison: initial price, maintenance, corrosion and downtime over 25 years.
FRP Resin Selection for Corrosion
Isophthalic, vinylester and phenolic resin — which to choose against acids, alkalis, chlorides and solvents.
FRP Grating Engineering Guide
Load/span calculation, deflection limits, clip schedules and support spacing for specifiers.
Specify Molded Grating for Your Platform?
Send us your dimensions and environment — we'll confirm availability and pricing within 24 hours. Whether your team writes fiberglass or fibreglass, the panels quoted are identical in construction and performance.
You may also like
Covered / Solid-Top FRP Grating
A solid FRP top plate bonded to a molded grating panel — 30% higher stiffness than open-mesh, while containing spills and blocking debris from falling through. Used for trench covers, odor-control zones, chemical secondary containment and food-plant washdown areas.
| Type | Construction | Best For |
|---|---|---|
| Covered gritted | 3 mm solid top + gritted walking surface | Wet/oily industrial walkways, drainage channels |
| Covered smooth | 3 mm solid top + smooth surface | Food & beverage washdown, odor control, trench covers |
| Covered concave | 3 mm solid top + concave dimples | H₂S condensate areas, chemical trenches |
Standards & Compliance
- ASTM F3059 — Standard Specification for Fiberglass-Reinforced Polymer (FRP) Gratings Used in Industrial Applications
- ASTM E84 — Surface Burning Characteristics (Class A available in phenolic / FR grades)
- BS 7976-2 / DIN 51130 — Slip resistance: gritted surfaces rated R13, concave meniscus R12
- ISO 24681:2023 — Maritime and marine environment FRP gratings (ship decks, ferry terminals)
- USCG / IMO FTP Code — Phenolic gratings accepted on shipboard and offshore installations
- BS EN 13501-1 — Reaction to fire: phenolic Class B-s1,d0
- BS EN 13700 — British / European Standard for pultruded GRP profiles; molded grating manufactured to EN 13700-2 specification
- ANSI/BHPA A117.1 / ADA — Mini-mesh 19×19 mm openings meet public-access opening limits
Molded FRP Grating Key Specifications & Applications
Molded FRP Grating Dimensions
Molded FRP grating dimensions: standard panel 1220x3660 mm (4x12 ft), thickness 25,30,38,50 mm. Custom cuts, notches and curved shapes available on request.
One-Piece Molded Grating
One-piece molded grating is compression-molded from continuous glass fiber and resin, giving bi-directional strength, uniform surface and no welded joints that can delaminate.
Molded Grating Mesh Sizes
Molded grating mesh sizes: 19x19 mm (mini-mesh, ADA-compliant), 38x38 mm (general walkway), 50x50 mm (debris-passing). Grit-top or concave meniscus anti-slip surfaces.
Pricing & Ordering
Price Reference, MOQ & Lead Time
Transparent pricing guide for standard GRP grating orders.
Price Reference (FOB Shanghai, USD/m²)
| Resin Type | Price Range (USD/m²) |
|---|---|
| Isophthalic Polyester (standard) | – |
| Vinyl Ester (corrosion-resistant) | – |
| Phenolic (fire-rated, low smoke) | – |
Surcharges: Mini-mesh 19×19mm (+20%), Heavy-duty 50mm (+50%), Custom colors (+10%).
MOQ & Lead Time
| Item | Details |
|---|---|
| Standard sizes MOQ | 50 m² |
| Custom sizes/colors MOQ | 100 m² |
| Sample order | 10 m² available |
| Stock items delivery | 7–10 working days |
| Custom sizes delivery | 20–25 working days |
| Large orders (500+ m²) | 30–40 working days |
Shipping: FOB Shanghai/Ningbo. Sea freight 15–35 days to most ports. Air freight available for urgent small orders.
Prices are reference only. Final pricing depends on quantity, resin type, mesh size, and customization. Contact us for an exact quote within 24 hours.
Looking for reliable molded FRP grating? ZeAllgrate has been manufacturing high-quality GRP grating since 2004, exporting to 45+ countries worldwide. Request a free sample or quote today.