ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

Standards & Compliance

ASTM, ISO 14122, OSHA 1910.23, ADA, NEMA and FM — clauses and scope

Test Methods

ASTM Material Test Methods

These are the standard mechanical and physical tests a compliant FRP material data sheet references.

StandardWhat It MeasuresTypical Use
ASTM D638Tensile properties (strength, modulus)Bearing-bar tensile data sheet
ASTM D790Flexural strength & modulusBeam stiffness, load/span design
ASTM D695Compressive propertiesEnd-bearing, crushing at supports
ASTM D792Density / specific gravityMass verification (kg/m²)
ASTM D570Water absorptionMoisture uptake, long-term exposure
ASTM D2583Barcol indentation hardnessSurface cure / quality check
ASTM E84Surface burning (flame spread & smoke)Fire class A/B/C
European & British Standards

BS EN 13700 — Pultruded GRP Profiles

ZeAllgrate pultruded and molded grating is manufactured to the British / European Standard for fibre-reinforced plastic (FRP/GRP) pultruded profiles, alongside the US ASTM and ISO test methods listed above.

StandardFull Title & ScopeZeAllgrate Compliance
BS EN 13700British / European Standard for pultruded GRP profiles. Covers pultruded GRP/FRP structural profiles and grating used in construction and industrial access.Manufactured in line with EN 13700-2 (specification for pultruded profiles); DoP and batch test reports available per order.
EN 13700-2Part 2: Specification for pultruded profiles — properties, tolerances and test methods for load-bearing GRP sections.Our pultruded I-bar, T-bar and rectangular grating profiles meet the dimensional and mechanical property clauses of EN 13700-2.
BS EN 13700 (molded grating)Reference scope extends to molded GRP grating panels used on European walkways, platforms and trench covers.Molded 38×38 mm, 19×19 mm mini-mesh and 50 mm heavy-duty panels supplied with EN-aligned load charts and deflection data.
ASTM E84Surface burning characteristics (flame spread & smoke development) — paired with BS EN 13501-1 reaction-to-fire in EU projects.Fire-retardant and phenolic grades: ASTM E84 Class B; reaction-to-fire Class B-s1,d0 on phenolic option.

For EU tenders, ZeAllgrate supplies a combined compliance pack covering BS EN 13700 / EN 13700-2, ASTM E84 Class B, ISO 14122 and OSHA 1910.23 — request it through the contact form.

Safety & Access

Platform, Access & Accessibility Codes

StandardScope & Key ClausesApplies To
ISO 14122 (parts 1–4)Permanent access to machinery. Part 3: stairs, stepladders and guard-rails; defines walkway width, pitch and guard systemsEuropean/ international fixed platforms
OSHA 29 CFR 1910.23Walking-working surfaces: guarding floor/wall openings, standard railings, toe boards and cover requirementsUS general industry platforms
ADA (Americans with Disabilities Act)Accessibility: accessible route surfaces, slip resistance (COF) and level walking surfacesPublic/accessible US facilities
NEMAElectrical/enclosure and fiberglass material standards; non-conductive applicationElectrical rooms, substations
FM Approval (fmGlobal)Insurance-driven approval of grating/construction for specific fire/hazard ratingsOffshore, high-hazard, insured sites

Related regional references: EN ISO 14122 (EU), AS 1657 (Australia), BS 4592 (UK). Always confirm the edition your project references.

Certification

What to Ask a Supplier for

Material Certificate

Glass content, resin type, panel dimensions, thickness, batch number — traceable to production records.

Load Test Report

Actual test panels, span, UDL/concentrated load and deflection — not extrapolated marketing data.

Fire Test Report

ASTM E84 FSI/SDI values, lab identity and product match for the grade shipped.

Standards Map at a Glance

AreaKey StandardsWhat ZeAllgrate Provides
Material testingASTM D790 (flexural), D2584 (burn-off), D2583 (hardness), C581 (chemical)Test reports for the exact grade
Fire performanceASTM E84 (flame spread / smoke)Class A/B/C report; confirm grade and thickness
Walking-working surfacesOSHA 29 CFR 1910.23 / 1910.28Load-tested handrail; load tables for grating
Fixed laddersOSHA 1910.23 / ISO 14122-4Rung spacing, load and cage systems
Access / platformsISO 14122-3Handrail, stairs and platform dimensions

What to Ask a Supplier

  • The test report for the exact resin and construction you are ordering — not a generic brochure value.
  • The load table basis (working vs ultimate) so the safety factor is not double-applied.
  • The E84 class for the grade and thickness, where fire rating is required.
  • Batch certificates matching the delivered panels for traceability.

Need a Compliance Package?

ZeAllgrate supplies certificates of conformity, load reports and E84 evidence — ask for your project file.

Source: ZeAllgrate (Fiberglass Grating Manufacturers Council / ACMA) design guidelines; ASTM International; ISO 14122; OSHA 29 CFR 1910. Indicative data for specification guidance only — final design verified by ZeAllgrate engineering against certified load/span charts.