ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

Fiberglass Fabric

E-glass woven roving · cloth · chopped strand mat For a broader overview of GRP grating types and specifications, see our technical guide.

Fiberglass Fabric
Product Overview

Fiberglass Fabric

High-performance E-glass fabrics are the reinforcement backbone of every composite part. ZeAllgrate supplies woven roving, plain weave cloth, biaxial fabrics and chopped strand mat for laminating, boat building, tank repair and structural reinforcement.

  • E-glass and C-glass grades
  • Woven roving: 400 – 1200 g/m²
  • Plain & twill weave cloth for smooth laminates
  • Biaxial / triaxial reinforcements for high-strength laminates
  • Chopped strand mat for tooling and surfacing
  • Consistent sizing chemistry for fast wet-out
Key Specifications

Technical Data

TypesWoven Roving / Cloth / CSM / Biaxial
Weight100 – 1200 g/m²
Width1000 / 1270 / 2000 mm
WeavePlain / Twill / Satin
GlassE-glass / ECR-glass
Roll Length50 / 100 m
Moisture< 0.2%
PackagingRolls with plastic wrap
Standard Configurations

Full Specification Matrix

Standard stocked configurations covering mesh, thickness, panel sizes and unit weights. Custom configurations available on request.

TypeWeight (g/m²)Width (mm)WeaveApplication
Woven Roving400 / 600 / 800 / 12001000 / 1270 / 2000PlainBoat hulls, tanks, laminating
E-Glass Cloth100 – 4001000 / 1270Plain / Twill / SatinSmooth laminates, tooling
Chopped Strand Mat300 – 9001000RandomSurfacing, tooling, repair
Biaxial600 – 120010000/90, ±45High-strength laminates
Triaxial800 – 160010000/90/±45Structural reinforcement

Values are standard industry configurations. Certified load/span charts and test reports provided with every order.

Material Properties

Physical & Mechanical Properties

Typical values tested in accordance with ASTM methods on production panels. Certified test reports available on request.

PropertyValueTest Method
Fiber TypeE-glass / C-glass—
Tensile Strength (woven roving)≥ 400 N/50mmGB/T 7689
Basis Weight Tolerance± 5%GB/T 9914.3
Moisture Content< 0.2%GB/T 9914.1
Sizing Content0.5 – 1.0%GB/T 9914.2
Product Gallery

In Production & In the Field

Real photographs from our manufacturing facility and installed projects.

Standards & Compliance

Engineered to International Standards

A

ASTM E84

Surface burning characteristics for fire-retardant grades — Class A/Class B options.

I

ISO 14122

Permanent means of access to machinery — platform, walkway and stair requirements.

S

AS 1657

Fixed platforms, walkways, stairways and ladders — design, construction and testing.

O

OSHA 1910

Walking-working surfaces and fall protection compliance for industrial installations.

Material certificates, load test reports and compliance documentation shipped with every order. Certified: ISO 9001:2015 · DNV & ABS Marine · SGS & Intertek. View certifications →

Surfaces & Colors

Options for Every Environment

SurfaceBest ForAnti-Slip
Concave / ConvexGeneral industrial walkways, platformsStandard molded profile
Grit-Top (Silica)Wet, oily and chemical process areasHigh — embedded silica grit
Micro-MeshPublic access, ADA-compliant small openingsHigh — small mesh profile
MeniscusLight pedestrian traffic, aestheticsModerate — meniscus surface

Standard colors: Green (RAL 6010), Gray (RAL 7047), Yellow (RAL 1003), Red, Blue, Black — custom Pantone/RAL matching available.

Chemical Resistance

Chemical Resistance Reference

Indicative chemical resistance by resin system — the basis of every material selection. Always confirm the final recommendation against our certified chemical resistance guide for your specific media, concentration and temperature.

Chemical MediumISO PolyesterVinyl EsterPhenolicService Notes
Sulfuric AcidGoodExcellentFairUp to 50%, 50 °C
Hydrochloric AcidGoodExcellentPoorUp to 37%, 50 °C
Sodium Hydroxide (Caustic)GoodGoodFairUp to 25%, 50 °C
Sodium Hypochlorite (Bleach)FairExcellentPoorUp to 15%, 40 °C
Hydrogen PeroxideFairGoodFairUp to 30%, 40 °C
Organic SolventsFairGoodPoorModerate temperature
Seawater / Salt SprayExcellentExcellentExcellentContinuous marine service
Petroleum / HydrocarbonsGoodExcellentFairModerate temperature
Acetic AcidGoodExcellentFairUp to 25%, 50 °C
Phosphoric AcidGoodExcellentFairUp to 85%, 60 °C

Ratings: Excellent — long-term service; Good — suitable with normal inspection; Fair — limited service, verify application. Full Chemical Resistance Guide →

Resin Systems

Ten Resin Systems for Every Chemical Environment

Corrosion resistance starts with the resin. ZeAllgrate manufactures in ten engineered resin systems, matching the industry’s proven material selection methodology.

Resin SystemKey PropertyMax Service TempTypical Use
Isophthalic Polyester (ISO)General corrosion resistance60 – 70 °CWater/wastewater, industrial floors
ISO Chemical GradeEnhanced chemical resistance70 – 80 °CChemical plant walkways
Vinyl Ester (VE)Superior acid/alkali/solvent resistance80 – 90 °CChemical, bleaching, pulp
VE Chemical GradeMaximum corrosion performance90 – 100 °CHarshest chemical exposure
PhenolicLow smoke, low flame spread120 – 150 °COffshore, fire-critical
Fire Retardant (FR)ASTM E84 Class B, flame spread ≤ 2560 – 70 °CCode-required flame ratings
UV-StabilizedOutdoor UV resistance60 – 70 °CSolar-exposed installations
Heat ResistantHigh-temperature service100 – 120 °CProcess heat areas
Conductive (Carbon)Static-dissipative60 – 70 °CElectrical / explosion areas
Food Grade (FDA)FDA-compliant contact surfaces60 – 70 °CFood & beverage processing

Our engineers prepare a written resin recommendation with every quotation — matched to your media, concentration and service temperature.

Installation

Installation Notes

✂

Cutting

Carbide-tipped or abrasive cutters; support both sides of the cut; wear dust protection. Wet cutting recommended.

🔩

Fastening

Fasten every panel at every support intersection. SS304/316 G-clips in corrosive service; expansion bolts for concrete.

↔

Orientation

Pultruded bearing bars run across the span — never parallel. Leave thermal gaps at fixed supports.

Installation ParameterRecommended PracticeStandard Reference
Support SpacingMaximum span per certified load chart — never exceed recommended clear spanLoad chart per configuration
BearingMinimum 40 mm bearing on each supportZeAllgrate practice / ISO 14122-3
Fastener SpacingMinimum 2 hold-down clips per support beam, spaced ≤ 1219 mm (4 ft) on centre; minimum 4 clips per panelPer ZeAllgrate engineering practice
Thermal ExpansionAllow 3 – 5 mm expansion gap at fixed supports; molded coefficient ≈ 15–25×10⁻⁶ /°C (direction dependent)Manufacturer data
Cut HolesSeal cut edges in chemical service with resin; radius corners to avoid stress pointsDesign guide
Fall ProtectionHandrail height ≥ 1100 mm (ISO 14122-3) / 42 in (OSHA 1910.23); kickplate where requiredOSHA 1910 / ISO 14122

Full Installation Guide →

Resin Systems

Choose the Right Resin for Your Environment

Corrosion resistance starts with the resin system. ZeAllgrate offers 3+ engineered resin systems for every chemical environment.

Isophthalic PolyesterGeneral-purpose corrosion resistance; excellent value for industrial and water/wastewater applications
Vinyl EsterSuperior chemical resistance to acids, alkalis and solvents — for chemical plants and bleaching environments
PhenolicLow smoke, low flame spread and high-temperature performance — for fire-critical and offshore applications
Fire-Retardant (FR)Enhanced flame-retardant grades meeting surface-burning requirements (ASTM E84)
UV-StabilizedUV-inhibited formulations for outdoor and solar-exposed installations

Contact our engineers for a chemical-resistance recommendation matched to your specific media, concentration and temperature.

Selection Process

How to Specify in Four Steps

1

Define Environment

Identify chemicals, temperature, UV exposure and load requirements.

2

Choose Grating Type

Molded for bi-directional strength; pultruded for long spans and heavy loads.

3

Check Load / Span

Verify the support span against certified load charts for your configuration.

4

Specify Surface & Clips

Grit-top for wet areas; SS304/316 clips for secure fastening.

Full Design Guide →

Technical Documents

Datasheets & Downloads

Fiberglass Fabric - Technical Data Sheet
PDF · Technical Document
PreviewDownload
ZeAllgrate Product Catalog
PDF · Technical Document
PreviewDownload
FRP Grating Design Guide
PDF · Technical Document
PreviewDownload
FAQ

Frequently Asked Questions

What is the lead time?

Standard panels: 7-15 days production; custom fabrication 15-20 days, plus shipping time. Urgent orders can be prioritized.

Can I get a free sample?

Yes - free small samples are available for evaluation. Contact sales@izeall.com with your application details.

What certificates do you provide?

Material certificates and load test reports are supplied with every shipment. Our facility is ISO 9001:2015 certified; marine grades carry DNV & ABS approvals, and third-party SGS & Intertek inspection and testing is available on request.

Related Technical Articles

Go Deeper with the ZeAllgrate Knowledge Base

📚

Manufacturing Process

Read article →

Molding and pultrusion — how fiber architecture drives strength.

📚

Glass Content & Fiber Architecture

Read article →

Roving, mat and woven layers explained.

📚

ISO Polyester Properties

Read article →

Resin matrix properties for composite reinforcement.

📚

Chemical Resistance & Resin Selection

Read article →

Corrosion performance of each resin system against aggressive media.

📚

Load & Span Tables

Read article →

Certified load classes and maximum clear spans by configuration.

📚

Grating Design Guide

Read article →

Support, bearing and expansion-gap design basics.

Need Fiberglass Fabrics in Bulk?

Send us your dimensions and environment — we'll confirm availability and pricing within 24 hours.