ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

Dock & Marina FRP Deck Grating

Saltwater-proof fiberglass decking for floating docks, piers and jetties For a broader overview of GRP grating types and specifications, see our technical guide.

FRP deck grating on marine dock
Why FRP for docks

FRP Deck Grating vs Wood and Steel

Dock decks see constant salt spray, standing water, UV sun and boat traffic. Wood rots and splinters; steel rusts. FRP deck grating in vinylester resin with SS316 clips survives 25+ years in marine service, is anti-slip when wet, and stays cool underfoot. Open area 65% lets wave splash drain immediately. See Marine & Coastal industry page.

Specs

Dock Deck Specs

ParameterValue
Panel#38 molded, vinylester
Weight14 kg/m²
ClipsSS316 C-clip
Anti-slipDouble carborundum
Life25+ years
Design

Marina Deck Design

Dock decks must (1) survive constant salt spray, (2) be anti-slip when wet, (3) be light enough for floating pontoons, (4) not rot. FRP molded #38 in vinylester resin is the standard marina decking. SS316 clips are mandatory (SS304 will pit in 2鈥? years). Double carborundum top for wet friction 0.8. Panel size 1220脳3660 mm; weight 14 kg/m² vs wood 18 kg/m² vs steel 48 kg/m².

Decking comparison

MaterialLifeMaintenanceWeight
FRP vinylester25+ yearsNone14 kg/m²
Hardwood (Ipe)10鈥?5 yearsOil annually18 kg/m²
Steel bar grating5鈥? yearsPaint every 3 years48 kg/m²
FAQ

Dock Deck FAQ

Can it be used on floating pontoons?

Yes. At 14 kg/m² it is lighter than wood, reducing pontoon buoyancy requirements.

Does it get hot in sun?

FRP has low thermal mass. White/gray colors stay cool. Dark colors get warm but not burning.

How do you fix to pontoon frame?

SS316 C-clips at 300 mm spacing. No through-bolts to the float chamber.

Marine specification

Marine Deck Specification

Marina decking must meet IMO Resolution A.753(18) for surface fire performance, and be resistant to salt spray per ASTM B117 (500 hours). Our vinylester molded #38 passes both. SS316 clips are mandatory 鈥?SS304 will pit in marine atmosphere within 2鈥? years. Anti-slip surface is double carborundum (top and bottom), giving wet friction 0.8 even when covered by seawater spray.

Floating vs fixed docks

On floating pontoons, weight is critical. FRP at 14 kg/m² is 70% lighter than steel grating, reducing pontoon buoyancy requirements by the same margin. On fixed piers, FRP decking is bolted to steel stringers with SS316 clips. See Marine & Coastal.

Why FRP

Why Engineers Choose GRP Over Steel

Glass-fiber reinforced polymer (GRP / FRP) grating has become the default choice for industrial walkways, platforms and trench covers. The reason is not aesthetics 鈥?it is total cost of ownership. Painted steel grating requires scraping and repainting every 3鈥? years in chemical and marine environments. Galvanized steel lasts 10鈥?5 years before corrosion attacks the bars. Aluminum corrodes in alkaline washdown areas. Stainless 316 is the only comparable metal, but at 3脳 the cost of vinylester GRP and still prone to pitting at the waterline.

FRP does not rust, does not need painting, and carries a 25-year design life. It is 70% lighter than steel, which reduces the structural steel subframe, lowers shipping cost, and makes manual installation feasible without heavy equipment. It is non-sparking and non-conductive, which is why it dominates refinery, offshore and substation applications. It also has a lower coefficient of thermal conductivity than aluminum, so barefoot areas stay cool in sunlight.

Total cost of ownership comparison

Cost item (25 years)Painted steel316 stainlessVinylester GRP
Initial material$25/m²$120/m²$45/m²
Repainting (every 4 yr)$60/m²$0$0
Replacement (15 yr)$25/m²$0$0
Subframe (lighter deck)$30/m²$30/m²$18/m²
25-year TCO$140/m²$150/m²$63/m²

The numbers tell the story: vinylester GRP is 55% lower total cost than either steel or stainless over a 25-year horizon. Add the safety benefits (non-sparking, non-conductive, anti-slip wet), and the engineering case is clear.

Ordering

How to Order: Specify, Draw, Deliver

We accept orders in three formats. (1) Standard catalog panels: 1220脳3660 mm, thickness 25/38/50 mm, shipped as-is. (2) Cut-to-size panels: send us a drawing with dimensions and cutouts, we fabricate to 卤3 mm tolerance. (3) Complete engineered package: we calculate loads, detail the subframe, produce assembly drawings, ship a numbered kit with all clips, bolts and handrail components. Typical lead time: 10 working days for standard panels, 20 working days for engineered packages.

What we need for a quote

  • Application (walkway / platform / trench / pool / dock, etc.)
  • Expected loads (pedestrian / trolley / vehicle)
  • Span between supports
  • Chemicals present (concentration and temperature)
  • Color requirement (standard gray / custom RAL)
  • Quantity in m²

Send us the spec and a hand sketch 鈥?we return a technical proposal with panel schedule, load table, and price within 48 hours. See our molded grating and pultruded grating product pages for detailed specs.

Maintenance

Installation and Lifetime Maintenance

FRP grating is famously low-maintenance. But "low maintenance" does not mean "no maintenance". For a 25-year service life, we recommend the following inspection schedule. Annual visual inspection: walk every 12 months, look for broken bars, missing clips, UV chalk on the top surface. Clips: re-torque every 3 years 鈥?thermal cycling loosens bolts slightly. Cleaning: wash with high-pressure water 200 bar; for chemical residue, use pH-neutral detergent. Do not use solvent-based cleaners on the gel coat 鈥?they can craze the surface.

UV chalk: after 8鈥?0 years outdoors, the gel coat may show faint surface chalk. This is normal and does not affect structural strength. If appearance matters, apply a coat of UV-stabilized clear gel coat, available from us as a touch-up kit. Repairs: a broken bar can be spliced with a FRP repair kit (resin + mat) in 30 minutes; the panel remains in service. Full panel replacement takes 15 minutes for two workers 鈥?no hot work, no welding.

Safety in installation

Cutting FRP generates dust. Wear P100 respirator, eye protection, gloves. Dust is silica-glass, not toxic but irritates lungs. Wet cutting suppresses dust. Do not cut near open flame 鈥?resin is combustible, though self-extinguishing per ASTM E84.

Specifications

Technical Specifications and Standards

Our GRP grating is manufactured under ISO 9001 quality system. Every batch is tested for flexural strength (ASTM E1310), water absorption (ASTM D570, <0.5%), bar size tolerance (卤0.5 mm), and resin content (65鈥?0% by weight). Fire performance per ASTM E84 Class B. Thermal stability per ISO 75 HDT (load deflection temperature) 鈥?180 掳C for vinylester. UV aging per ASTM G154 (1000 hours QUV) 鈥?gt;70% retained strength.

StandardScope
BS 4592 Part 4GRP grating specifications
EN ISO 14122-2/3Permanent access to machinery
ASTM E84Surface burning characteristics
ASTM E1310FRP grating test method
ASTM G154UV fluorescent aging
ISO 75Heat deflection temperature

See also FRP grating clips, FRP grating covers, and FRP structural profiles for complementary products.

Selection guide

Choosing the Right GRP Panel

When specifying GRP grating for a new project, three variables dominate: panel thickness, resin type, and surface finish. Thickness carries the load. Resin determines chemical and temperature resistance. Surface finish determines slip resistance. Get these three right and the rest follows.

Panel thickness guide

PanelWeightTypical spanUse
#25 molded9 kg/m²600 mmLight walkway, solar, tree grate
#38 molded14 kg/m²900 mmStandard industrial platform
#50 molded22 kg/m²1200 mmCart traffic, heavy duty
I 40 pultruded8 kg/m²900 mmHigh load, light weight
I 50 pultruded12 kg/m²1200 mmLong span, trolley
I 75 pultruded18 kg/m²1800 mmHeavy, equipment access

Resin selection

Isophthalic is the default for atmospheric and light chemical service. Vinylester for marine, chemical splash, hot water. Phenolic for high temperature and low-smoke requirements. We provide a chemical resistance chart for 200+ chemicals on request 鈥?if your media is not listed, send us the concentration and temperature, and our engineering team will recommend the right resin.

Surface finish

Smooth top for indoor dry areas. Carborundum grit (aluminum oxide F24) for wet and slip-prone areas. Double grit (top and bottom) for marine and washdown. The grit is cast into the gel coat, not glued on 鈥?it will not peel.

Why ZeAllgrate

About ZeAllgrate Manufacturing

ZeAllgrate is a China-based manufacturer of FRP / GRP grating since 2004. Our 15,000 m² factory has an annual capacity of 200,000 m² of molded and pultruded grating. We export to 45+ countries: Europe, North America, Middle East, Southeast Asia. Every batch is ISO 9001 certified, ASTM E84 tested, and ships with Mill Test Certificate. Our engineering team supports your spec from sketch to installation drawing.

We are not a trading company 鈥?we are the factory. That means direct pricing, fast lead time (10 days for standard panels), and technical support from the people who made the product. Contact our engineering team for your next FRP project.

Send us dock layout

We return decking take-off with clip schedule.