ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

Custom FRP Pultrusion

OEM · ODM · custom profiles pultruded to print For a broader overview of GRP grating types and specifications, see our technical guide.

Custom FRP pultrusion profile manufactured to OEM drawing
Product Overview

Custom FRP Pultrusion

Custom FRP pultrusion is how ZeAllgrate turns your drawing into a production fiberglass profile. Using in-house pultrusion tooling and custom steel dies, we produce made-to-print structural shapes, OEM components and fully assembled sub-systems — with glass contents, resin systems and tolerances engineered for your application. Our pultrusion FRP profiles line turns out pultruded fiberglass profiles and pultruded GRP sections to print.

  • Custom dies & tooling — profile shapes to your cross-section
  • In-house pultrusion with 60–75% E-glass / glass content control
  • OEM & ODM: private-label, kitted sub-assemblies, co-development
  • Resin systems: ISO / Vinyl Ester / Phenolic / FR / Conductive
  • Tolerances per drawing; machining, drilling & cut-to-length
  • Low MOQ friendly; NDA-protected design confidentiality
Applications

From Profile to Production-Ready Part

ZeAllgrate carries out custom pultrusion for OEMs, engineering firms and project contractors who need a dedicated FRP shape rather than an off-the-shelf profile. Typical parts are an industrial frame, machine guard, cable tray or purlin roof framing; as an FRP profiles manufacturer, pultruded profiles supplier and GRP sections factory, we act as your custom supplier and exporter for made-to-print composite sections.

Open-mesh FRP grating cover for trench and drain
Custom Structural Shapes

I-beams, channels, tubes, angles and closed sections pultruded to your cross-section — replacing steel with corrosion-proof composite at the same design stiffness.

Solid FRP cover panel with sealed gritted surface for tank and trench covers
OEM Components & Sub-Assemblies

Brackets, frames, cable trays, ladder sections and kitted parts produced under OEM/ODM programs, private-labelled and supplied just-in-time to your spec.

Every pultrusion is made to print with certified material properties. Send us your drawing for a quote →

Key Specifications

Technical Data

TypeCustom Pultruded FRP Profiles / OEM Components
MaterialMolded or Pultruded FRP
Glass Content60 – 75% E-glass (unidirectional / mat hybrid)
Load ClassA15 / B125 / C250 / D400 / E600 / F900
Panel SizeCross-section to print; cut-to-length any
FrameMachined / drilled / bolted per assembly
HardwareSS304 / SS316
ColorsGrey / Red / Yellow / Green (custom RAL/Pantone)
SurfaceGrit-top / Plain
LockingPadlock / bolt-down optional
Engineering Drawings

Product Drawings & Details

Dimensioned drawings for specification and fabrication — matching the technical documentation of leading FRP manufacturers.

DW-01 G-Clip Fastening — Section
DWG NO: ZL-XDG-01SCALE 1:10UNITS: mmMAT: FRPFRP gratingSupport beamG-clip≥40 mm3–5 mmSS304/316 or FRP clip; min 2 clips per support beam
DW-02 Edge Trim & Cut Edge Sealing
DWG NO: ZL-XDG-02SCALE 1:10UNITS: mmMAT: FRPGrating panelEdge trimSupportCut edges sealed with polyester resin
DW-03 Stair Tread Fixing
DWG NO: ZL-XDG-03SCALE 1:10UNITS: mmMAT: FRPTread w/ nosepieceTread fixed to stringer with SS fasteners
DW-04 Expansion Joint Detail
DWG NO: ZL-XDG-04SCALE 1:10UNITS: mmMAT: FRP3–5 mmContinuous supportExpansion gap at every fixed support
Standard Configurations

Pultrusion Capability Reference

Typical pultrusion capability envelope — verify exact properties against certified test data for your profile.

Load ClassRated LoadTypical ServiceRecommended Use
Standard shapes100+ stock diesI-beam, channel, angle, tube, barGeneral structure, OEM
Custom cross-sectionNew die & toolingMade to your printOEM / proprietary shapes
Continuous lengthCut to lengthUp to 12 m (longer on request)Beams, stringers
A1515 kNPedestrian onlyFootpaths, inspection covers
B125125 kNSidewalks, light vehiclesSidewalks, car parks
C250250 kNVehicle areas (slow)Trench covers, service roads
D400400 kNHeavy vehicle areasLoading docks, industrial yards
E600600 kNForklift / industrialIndustrial floors, warehouses
F900900 kNExtreme industrialRunways, special heavy service

Values are standard industry configurations. Certified load/span charts and test reports provided with every order.

Material Properties

Physical & Mechanical Properties

Typical values tested in accordance with ASTM methods on production panels. Certified test reports available on request.

PropertyValueTest Method
Tensile Strength70 – 220 MPaASTM D638
Flexural Strength110 – 240 MPaASTM D790
Compressive Strength170 – 240 MPaASTM D695
Flexural Modulus8 – 13 GPaASTM D790
Density1.7 – 1.9 g/cm³ASTM D792
Water Absorption (24h)< 0.5%ASTM D570
Flame Spread≤ 25 (Class A)ASTM E84
Product Gallery

In Production & In the Field

Real photographs from our manufacturing facility and installed projects.

Standards & Compliance

Engineered to International Standards

A

ASTM E84

Surface burning characteristics for fire-retardant grades — Class A/Class B options.

I

ISO 14122

Permanent means of access to machinery — platform, walkway and stair requirements.

S

AS 1657

Fixed platforms, walkways, stairways and ladders — design, construction and testing.

O

OSHA 1910

Walking-working surfaces and fall protection compliance for industrial installations.

Material certificates, load test reports and compliance documentation shipped with every order. Certified: ISO 9001:2015 · DNV & ABS Marine · SGS & Intertek. View certifications →

Surfaces & Colors

Options for Every Environment

SurfaceBest ForAnti-Slip
Concave / ConvexGeneral industrial walkways, platformsStandard molded profile
Grit-Top (Silica)Wet, oily and chemical process areasHigh — embedded silica grit
Micro-MeshPublic access, ADA-compliant small openingsHigh — small mesh profile
MeniscusLight pedestrian traffic, aestheticsModerate — meniscus surface

Standard colors: Green (RAL 6010), Gray (RAL 7047), Yellow (RAL 1003), Red, Blue, Black — custom Pantone/RAL matching available.

Chemical Resistance

Chemical Resistance Reference

Indicative chemical resistance by resin system — the basis of every material selection. Always confirm the final recommendation against our certified chemical resistance guide for your specific media, concentration and temperature.

Chemical MediumISO PolyesterVinyl EsterPhenolicService Notes
Sulfuric AcidGoodExcellentFairUp to 50%, 50 °C
Hydrochloric AcidGoodExcellentPoorUp to 37%, 50 °C
Sodium Hydroxide (Caustic)GoodGoodFairUp to 25%, 50 °C
Sodium Hypochlorite (Bleach)FairExcellentPoorUp to 15%, 40 °C
Hydrogen PeroxideFairGoodFairUp to 30%, 40 °C
Organic SolventsFairGoodPoorModerate temperature
Seawater / Salt SprayExcellentExcellentExcellentContinuous marine service
Petroleum / HydrocarbonsGoodExcellentFairModerate temperature
Acetic AcidGoodExcellentFairUp to 25%, 50 °C
Phosphoric AcidGoodExcellentFairUp to 85%, 60 °C

Ratings: Excellent — long-term service; Good — suitable with normal inspection; Fair — limited service, verify application. Full Chemical Resistance Guide →

Resin Systems

Ten Resin Systems for Every Chemical Environment

Corrosion resistance starts with the resin. ZeAllgrate manufactures in ten engineered resin systems, matching the industry’s proven material selection methodology.

Resin SystemKey PropertyMax Service TempTypical Use
Isophthalic Polyester (ISO)General corrosion resistance60 – 70 °CWater/wastewater, industrial floors
ISO Chemical GradeEnhanced chemical resistance70 – 80 °CChemical plant walkways
Vinyl Ester (VE)Superior acid/alkali/solvent resistance80 – 90 °CChemical, bleaching, pulp
VE Chemical GradeMaximum corrosion performance90 – 100 °CHarshest chemical exposure
PhenolicLow smoke, low flame spread120 – 150 °COffshore, fire-critical
Fire Retardant (FR)ASTM E84 Class B, flame spread ≤ 2560 – 70 °CCode-required flame ratings
UV-StabilizedOutdoor UV resistance60 – 70 °CSolar-exposed installations
Heat ResistantHigh-temperature service100 – 120 °CProcess heat areas
Conductive (Carbon)Static-dissipative60 – 70 °CElectrical / explosion areas
Food Grade (FDA)FDA-compliant contact surfaces60 – 70 °CFood & beverage processing

Our engineers prepare a written resin recommendation with every quotation — matched to your media, concentration and service temperature.

Installation

Installation Notes

✂

Cutting

Carbide-tipped or abrasive cutters; support both sides of the cut; wear dust protection. Wet cutting recommended.

🔩

Fastening

Fasten every panel at every support intersection. SS304/316 G-clips in corrosive service; expansion bolts for concrete.

↔

Orientation

Pultruded bearing bars run across the span — never parallel. Leave thermal gaps at fixed supports.

Installation ParameterRecommended PracticeStandard Reference
Support SpacingMaximum span per certified load chart — never exceed recommended clear spanLoad chart per configuration
BearingMinimum 40 mm bearing on each supportZeAllgrate practice / ISO 14122-3
Fastener SpacingMinimum 2 hold-down clips per support beam, spaced ≤ 1219 mm (4 ft) on centre; minimum 4 clips per panelPer ZeAllgrate engineering practice
Thermal ExpansionAllow 3 – 5 mm expansion gap at fixed supports; molded coefficient ≈ 15–25×10⁻⁶ /°C (direction dependent)Manufacturer data
Cut HolesSeal cut edges in chemical service with resin; radius corners to avoid stress pointsDesign guide
Fall ProtectionHandrail height ≥ 1100 mm (ISO 14122-3) / 42 in (OSHA 1910.23); kickplate where requiredOSHA 1910 / ISO 14122

Full Installation Guide →

Resin Systems

Choose the Right Resin for Your Environment

Corrosion resistance starts with the resin system. ZeAllgrate offers 3+ engineered resin systems for every chemical environment.

Isophthalic PolyesterGeneral-purpose corrosion resistance; excellent value for industrial and water/wastewater applications
Vinyl EsterSuperior chemical resistance to acids, alkalis and solvents — for chemical plants and bleaching environments
PhenolicLow smoke, low flame spread and high-temperature performance — for fire-critical and offshore applications
Fire-Retardant (FR)Enhanced flame-retardant grades meeting surface-burning requirements (ASTM E84)
UV-StabilizedUV-inhibited formulations for outdoor and solar-exposed installations

Contact our engineers for a chemical-resistance recommendation matched to your specific media, concentration and temperature.

Selection Process

How to Specify in Four Steps

1

Define Environment

Identify chemicals, temperature, UV exposure and load requirements.

2

Choose Grating Type

Molded for bi-directional strength; pultruded for long spans and heavy loads.

3

Check Load / Span

Verify the support span against certified load charts for your configuration.

4

Specify Surface & Clips

Grit-top for wet areas; SS304/316 clips for secure fastening.

Full Design Guide →

Technical Documents

Datasheets & Downloads

Custom FRP Pultrusion - Technical Data Sheet
PDF · Technical Document
PreviewDownload
ZeAllgrate Product Catalog
PDF · Technical Document
PreviewDownload
FRP Grating Design Guide
PDF · Technical Document
PreviewDownload
FAQ

Frequently Asked Questions

What is the lead time?

Standard panels: 7-15 days production; custom fabrication 15-20 days, plus shipping time. Urgent orders can be prioritized.

Can I get a free sample?

Yes - free small samples are available for evaluation. Contact sales@izeall.com with your application details.

What certificates do you provide?

Material certificates and load test reports are supplied with every shipment. Our facility is ISO 9001:2015 certified; marine grades carry DNV & ABS approvals, and third-party SGS & Intertek inspection and testing is available on request.

Related Technical Articles

Go Deeper with the ZeAllgrate Knowledge Base

📚

Grating Cover Selection

Read article →

Choosing covers by load class, traffic and environment.

📚

Trench Cover Load Ratings

Read article →

Load-rated trench, basin and screening covers.

📚

Load & Span Charts

Read article →

Reading certified load/span tables for cover panels.

📚

Chemical Resistance & Resin Selection

Read article →

Corrosion performance of each resin system against aggressive media.

📚

Load & Span Tables

Read article →

Certified load classes and maximum clear spans by configuration.

📚

Grating Design Guide

Read article →

Support, bearing and expansion-gap design basics.

Custom

Custom / Special-Shaped Pultrusions

Custom and special-shaped pultrusions are produced from customer drawings: bespoke cross-sections, co-extruded colours, integrated grooves and reinforcement lay-ups. Send the drawing and load case — engineering returns a tooled pultrusion section matched to the duty.

Need a Custom Pultrusion?

Send your drawing or cross-section — our engineers will confirm feasibility, tooling cost and lead time within 24 hours.