GRP grating and FRP grating are the standard decking choice for rail and metro infrastructure where stray current, third-rail voltage and de-icing salts make steel a liability. ZeAllgrate supplies non-conductive fiberglass panels for platform edges, trackside catwalks and cable trough covers. For a broader overview see our GRP grating technical guide.

GRP grating panels installed as railway platform walkway
Why GRP for rail

Non-Conductive Decking for Electrified Rail

Electrified railways carry 750 V DC third rail or 25 kV AC overhead supply. Steel walkways and trench covers become part of the electrical circuit — a fault can energize the entire platform edge. GRP grating is dielectric: surface resistance above 10¹² Ω·cm breaks the conductive path and protects maintenance staff and passengers. FRP grating also does not corrode from de-icing salts, brake dust and tunnel condensation, which eat through painted steel in 3–5 years.

At 14 kg/m² for a 38 mm molded panel, GRP grating is roughly one-quarter the weight of steel bar grating. A two-person crew can lift and position a 1.22 × 3.66 m panel without a track crane, which is decisive in night possessions where every minute counts. Panels cut with hand tools — no hot work, no welding permits on the electrified corridor.

  • Dielectric — safe over third rail and 25 kV catenary zones
  • Lightweight — install by hand during short track possessions
  • Salt & brake-dust resistant — no rust in tunnels and stations
  • Non-sparking — approved for under-track and depot areas
Grades

Railway-Grade GRP Grating Selection

Choose the resin and panel to match the exposure. For tunnel and underground stations specify phenolic resin for low smoke and flame spread.

LocationResinPanelMax span (pedestrian)
Platform edge / concourseIsophthalic#38 molded900 mm
Trackside catwalkVinylester#38 molded900 mm
Cable trough coverVinylester#50 molded / coveredper EN 124
Underground / tunnelPhenolic#38 molded750 mm

Low-smoke phenolic grade is required per EN 45545 for rolling stock and underground stations. Contact us for EN 45545-2 R24 / HL3 certification documentation.

Applications

Where FRP Grating Is Used on the Rail Network

Platform edge walkways

Dielectric decking over third rail and platform gaps.

Trackside catwalks

Lightweight panels for night maintenance works.

Cable trough covers

Lockable, anti-slip FRP grating over signal cables.

Depot & workshop floors

Oil and brake-fluid resistant wash decks.

Ventilation openings

Secure rat-proof GRP grating over duct shafts.

Pedestrian crossing decks

Grit-top anti-slip in rain and leaf fall.

Safety

Why Engineers Specify FRP Grating Over Steel for Railways

Stray current protection is the decisive technical driver. In DC electrified systems, leakage current returns through the running rails. Any conductive metalwork bonded to the rail can carry that current, causing electrolytic corrosion of buried services and shock risk to staff. GRP grating and FRP grating are inherently insulating, so they cannot conduct stray current — no bonding cables, no insulation joints, no ongoing testing regime.

Corrosion from de-icing salts (calcium chloride, magnesium chloride) and tunnel humidity destroys steel grating in under five years. GRP grating in vinylester or phenolic resin is immune, and carries a 25-year design life. The panels also carry a carborundum grit top to keep platform edges safe when wet or during leaf-fall season.

PropertySteel gratingGRP / FRP grating
Weight (38 mm panel)~45 kg/m²~14 kg/m²
ElectricalConductive>10¹² Ω·cm dielectric
De-icing salt life3–5 years25 years
Hot work on siteRequiredNone — hand tools only
FAQ

Rail GRP Grating FAQ

Is GRP grating safe near the third rail?

Yes — it is dielectric with surface resistance above 10¹² Ω·cm and is widely used as cover and walkway over energized third rail. Always isolate the circuit during installation regardless of material.

What panel thickness is used for platform walkways?

#38 molded GRP grating (38 mm) on 900 mm supports for standard pedestrian platforms; #50 molded FRP grating for equipment trolley routes.

Can cable trough covers be locked?

Yes — we supply covered FRP grating trough panels with SS316 lockable bolts and lifting keys, rated per EN 124 load classes for public areas.

Does it meet fire rules for underground metro?

Phenolic GRP grating meets EN 45545-2 low-smoke, low-toxicity requirements for tunnels and underground stations; vinylester grade is for open-air trackside.