ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

ZeAllgrate FRP Molded Grating

Bi-directional strength · anti-slip · corrosion resistant

ZeAllgrate FRP Molded Grating
Product Overview

ZeAllgrate FRP Molded Grating

ZeAllgrate molded grating is manufactured in a compression molding process that interlocks continuous glass fibers in two directions, delivering exceptional bi-directional strength and impact resistance. It is the world's most widely specified FRP grating — and ours is engineered for the harshest service conditions.

  • Bi-directional strength: equal load capacity in both panel directions
  • Anti-slip surfaces: concave/convex, grit-top (silica) options
  • 3+ resin systems: isophthalic, vinyl ester, phenolic, fire-retardant
  • Panel sizes up to 1220 × 3660 mm; thickness 25 / 30 / 38 / 40 / 50 mm
  • Non-conductive, non-magnetic, spark-resistant
  • Service life 20+ years with zero maintenance in corrosive service

Also available as trench, basin & screening covers →

Key Specifications

Technical Data

Standard Panel1220 × 3660 mm (4' × 12')
Thickness25 / 30 / 38 / 40 / 50 mm
Mesh Pitch38×38 / 40×40 / 50×50 mm
Glass Content33% ± 3% (molded)
SurfaceConcave / Convex / Grit-top
Resin SystemsISO Polyester / Vinyl Ester / Phenolic / Fire-Retardant
ColorsGreen, Gray, Yellow, Red, Blue, Custom
Load TestPer ASTM E84, ISO 14122
Engineering Drawings

Product Drawings & Details

Dimensioned drawings for specification and fabrication — matching the technical documentation of leading FRP manufacturers.

DW-01 Plan View — 38.1 × 38.1 mm Mesh, 31 mm Opening
DWG NO: ZL-MDG-01SCALE 1:10UNITS: mmMAT: FRP38.1 mm38.1 mm31 mmLoad bar (amber) interlocks cross bars (gray) — equal capacity both ways
DW-02 Section A-A — Meniscus (Concave) Top Profile, 25.4 mm Deep
DWG NO: ZL-MDG-02SCALE 1:10UNITS: mmMAT: FRPMeniscus concave anti-slip top — standard molded surface25.4 mm6.4 mm(1/4 in load bar)38.1 mm pitch
DW-03 Section B-B — Cross Bar Interlock Detail
DWG NO: ZL-MDG-03SCALE 1:10UNITS: mmMAT: FRPTie bar 6.4 mm (1/4 in)6.4 mm31 mmLoad bar interlocks tie bar — equal capacity both ways
DW-04 Installation — Support & Fastening
DWG NO: ZL-MDG-04SCALE 1:10UNITS: mmMAT: FRPFRP gratingSupport beamG-clipSS304/316≥40 mm3–5 mm gap3–5 mm expansion gap at fixed supports
Standard Configurations

Full Specification Matrix

Standard stocked configurations covering mesh, thickness, panel sizes and unit weights. Custom configurations available on request.

ThicknessMesh PatternPanel Sizes (m)Open AreaWeight (kg/m²)
25.4 mm38.1 × 38.1 mm square0.91 × 3.05 / 1.22 × 3.6670%12.7
25.4 mm25.4 × 101.6 mm rectangular0.91 × 3.05 / 1.22 × 3.6669%13.7
38.1 mm38.1 × 38.1 mm square0.91 × 3.05 / 1.52 × 3.05 / 1.22 × 3.66 / 1.52 × 3.6670%18.6
38.1 mmMini-Mesh 19.05 × 19.05 top, 38.1 × 38.1 bottom1.22 × 3.6644%22.0
50.8 mm50.8 × 50.8 mm square1.22 × 3.6672%19.5
25.4 mmMicro-Mesh 19.05 × 19.05 top, 38.1 × 38.1 bottom1.22 × 3.6644%14.2
38.1 mmHLC 25.4 × 50.8 mm rectangular1.22 × 3.6648%30.3
50.8 mmHLC 25.4 × 50.8 mm rectangular1.22 × 3.6648%41.0

Values are standard industry configurations. Certified load/span charts and test reports provided with every order.

Load Reference

Load & Span Reference Table

Indicative allowable loads by span. Verify final design against certified load charts for your exact configuration.

SpanCL 25 mmCL 38 mmCL 50 mmUDL 25 mmUDL 38 mmUDL 50 mm
460 mm412 kgf564 kgf1,161 kgf2,600 kgf/m²3,400 kgf/m²5,200 kgf/m²
610 mm240 kgf377 kgf732 kgf1,900 kgf/m²2,500 kgf/m²3,800 kgf/m²
915 mm120 kgf167 kgf341 kgf900 kgf/m²1,200 kgf/m²1,900 kgf/m²
1220 mm60 kgf92 kgf197 kgf480 kgf/m²640 kgf/m²1,000 kgf/m²
Material Properties

Physical & Mechanical Properties

Typical values tested in accordance with ASTM methods on production panels. Certified test reports available on request.

PropertyValueTest Method
Tensile Strength70 MPaASTM D638
Flexural Strength110 MPaASTM D790
Compressive Strength170 MPaASTM D695
Flexural Modulus8 GPaASTM D790
Density1.7 g/cm³ASTM D792
Water Absorption (24h)< 0.5%ASTM D570
Barcol Hardness40 – 50ASTM D2583
Flame Spread≤ 25 (Class A)ASTM E84
Section Properties

Section Properties per Unit Width

Area (A), moment of inertia (I) and section modulus (S) per metre of panel width — for structural design of platforms and walkways.

ConfigurationDepthMeshA (mm²/m)I (×10⁶ mm⁴/m)S (×10³ mm³/m)
Std 25.425.4 mm38.1 × 38.1 sq3.62 × 10³0.19115.6
Std 25.4 R25.4 mm25.4 × 101.6 rect5.44 × 10³0.30023.1
Std 38.138.1 mm38.1 × 38.1 sq6.03 × 10³0.69634.9
Mini-Mesh 38.138.1 mm19.05 / 38.17.98 × 10³0.97542.6
Std 50.850.8 mm50.8 × 50.8 sq6.09 × 10³1.31150.5

Indicative design values. Structural design should be verified by a qualified engineer against certified section data for the exact resin and configuration.

Product Gallery

In Production & In the Field

Real photographs from our manufacturing facility and installed projects.

Factory Tour

See How ZeAllgrate Is Made

Compression molding & pultrusion lines at our Qidong facility — ISO 9001:2015 certified.

Standards & Compliance

Engineered to International Standards

A

ASTM E84

Surface burning characteristics for fire-retardant grades — Class A/Class B options.

I

ISO 14122

Permanent means of access to machinery — platform, walkway and stair requirements.

S

AS 1657

Fixed platforms, walkways, stairways and ladders — design, construction and testing.

O

OSHA 1910

Walking-working surfaces and fall protection compliance for industrial installations.

Material certificates, load test reports and compliance documentation shipped with every order. Certified: ISO 9001:2015 · DNV & ABS Marine · SGS & Intertek. View certifications →

Surfaces & Colors

Options for Every Environment

SurfaceBest ForAnti-Slip
Concave / ConvexGeneral industrial walkways, platformsStandard molded profile
Grit-Top (Silica)Wet, oily and chemical process areasHigh — embedded silica grit
Micro-MeshPublic access, ADA-compliant small openingsHigh — small mesh profile
MeniscusLight pedestrian traffic, aestheticsModerate — meniscus surface

Standard colors: Green (RAL 6010), Gray (RAL 7047), Yellow (RAL 1003), Red, Blue, Black — custom Pantone/RAL matching available.

Chemical Resistance

Chemical Resistance Reference

Indicative chemical resistance by resin system — the basis of every material selection. Always confirm the final recommendation against our certified chemical resistance guide for your specific media, concentration and temperature.

Chemical MediumISO PolyesterVinyl EsterPhenolicService Notes
Sulfuric AcidGoodExcellentFairUp to 50%, 50 °C
Hydrochloric AcidGoodExcellentPoorUp to 37%, 50 °C
Sodium Hydroxide (Caustic)GoodGoodFairUp to 25%, 50 °C
Sodium Hypochlorite (Bleach)FairExcellentPoorUp to 15%, 40 °C
Hydrogen PeroxideFairGoodFairUp to 30%, 40 °C
Organic SolventsFairGoodPoorModerate temperature
Seawater / Salt SprayExcellentExcellentExcellentContinuous marine service
Petroleum / HydrocarbonsGoodExcellentFairModerate temperature
Acetic AcidGoodExcellentFairUp to 25%, 50 °C
Phosphoric AcidGoodExcellentFairUp to 85%, 60 °C

Ratings: Excellent — long-term service; Good — suitable with normal inspection; Fair — limited service, verify application. Full Chemical Resistance Guide →

Resin Systems

Ten Resin Systems for Every Chemical Environment

Corrosion resistance starts with the resin. ZeAllgrate manufactures in ten engineered resin systems, matching the industry’s proven material selection methodology.

Resin SystemKey PropertyMax Service TempTypical Use
Isophthalic Polyester (ISO)General corrosion resistance60 – 70 °CWater/wastewater, industrial floors
ISO Chemical GradeEnhanced chemical resistance70 – 80 °CChemical plant walkways
Vinyl Ester (VE)Superior acid/alkali/solvent resistance80 – 90 °CChemical, bleaching, pulp
VE Chemical GradeMaximum corrosion performance90 – 100 °CHarshest chemical exposure
PhenolicLow smoke, low flame spread120 – 150 °COffshore, fire-critical
Fire Retardant (FR)ASTM E84 Class A, flame spread ≤ 2560 – 70 °CCode-required flame ratings
UV-StabilizedOutdoor UV resistance60 – 70 °CSolar-exposed installations
Heat ResistantHigh-temperature service100 – 120 °CProcess heat areas
Conductive (Carbon)Static-dissipative60 – 70 °CElectrical / explosion areas
Food Grade (FDA)FDA-compliant contact surfaces60 – 70 °CFood & beverage processing

Our engineers prepare a written resin recommendation with every quotation — matched to your media, concentration and service temperature.

Installation

Installation Notes

✂

Cutting

Carbide-tipped or abrasive cutters; support both sides of the cut; wear dust protection. Wet cutting recommended.

🔩

Fastening

Fasten every panel at every support intersection. SS304/316 G-clips in corrosive service; expansion bolts for concrete.

↔

Orientation

Pultruded bearing bars run across the span — never parallel. Leave thermal gaps at fixed supports.

Installation ParameterRecommended PracticeStandard Reference
Support SpacingMaximum span per certified load chart — never exceed recommended clear spanLoad chart per configuration
BearingMinimum 40 mm bearing on each supportZeAllgrate practice / ISO 14122-3
Fastener SpacingMinimum 2 hold-down clips per support beam, spaced ≤ 1219 mm (4 ft) on centre; minimum 4 clips per panelPer ZeAllgrate engineering practice
Thermal ExpansionAllow 3 – 5 mm expansion gap at fixed supports; molded coefficient ≈ 15–25×10⁻⁶ /°C (direction dependent)Manufacturer data
Cut HolesSeal cut edges in chemical service with resin; radius corners to avoid stress pointsDesign guide
Fall ProtectionHandrail height ≥ 1100 mm (ISO 14122-3) / 42 in (OSHA 1910.23); kickplate where requiredOSHA 1910 / ISO 14122

Full Installation Guide →

Resin Systems

Choose the Right Resin for Your Environment

Corrosion resistance starts with the resin system. ZeAllgrate offers 3+ engineered resin systems for every chemical environment.

Isophthalic PolyesterGeneral-purpose corrosion resistance; excellent value for industrial and water/wastewater applications
Vinyl EsterSuperior chemical resistance to acids, alkalis and solvents — for chemical plants and bleaching environments
PhenolicLow smoke, low flame spread and high-temperature performance — for fire-critical and offshore applications
Fire-Retardant (FR)Enhanced flame-retardant grades meeting surface-burning requirements (ASTM E84)
UV-StabilizedUV-inhibited formulations for outdoor and solar-exposed installations

Contact our engineers for a chemical-resistance recommendation matched to your specific media, concentration and temperature.

Selection Process

How to Specify in Four Steps

1

Define Environment

Identify chemicals, temperature, UV exposure and load requirements.

2

Choose Grating Type

Molded for bi-directional strength; pultruded for long spans and heavy loads.

3

Check Load / Span

Verify the support span against certified load charts for your configuration.

4

Specify Surface & Clips

Grit-top for wet areas; SS304/316 clips for secure fastening.

Full Design Guide →

Technical Documents

Datasheets & Downloads

FRP Molded Grating - Technical Data Sheet
PDF · Technical Document
Download
ZeAllgrate Product Catalog
PDF · Technical Document
Download
FRP Grating Design Guide
PDF · Technical Document
Download
FAQ

Frequently Asked Questions

What is the lead time?

Standard panels: 7-15 days production; custom fabrication 15-20 days, plus shipping time. Urgent orders can be prioritized.

Can I get a free sample?

Yes - free small samples are available for evaluation. Contact sales@izeall.com with your application details.

What certificates do you provide?

Material certificates and load test reports are supplied with every shipment. Our facility is ISO 9001:2015 certified; marine grades carry DNV & ABS approvals, and third-party SGS & Intertek inspection and testing is available on request.

Related Technical Articles

Go Deeper with the ZeAllgrate Knowledge Base

📚

Molded vs. Pultruded Grating

When to choose bi-directional molded or unidirectional pultruded strength.

Read article →
📚

Load & Deflection Selection

Match load class and span to panel stiffness and deflection limits.

Read article →
📚

Anti-Slip Surfaces Compared

Grit-top, concave and silica-cast surfaces and their slip ratings.

Read article →
📚

Installation Tips

Clips, cutting, expansion gaps and common field mistakes.

Read article →

Specify Molded Grating for Your Platform?

Send us your dimensions and environment — we'll confirm availability and pricing within 24 hours.