ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

Pultruded Grating — Full Profile Catalog & Section Properties

Complete bearing-bar catalog (I-bar / T-bar), assembled mesh configurations, section properties, tie-bar options and span reference.

Manufacturing & Design Basis

Pultruded FRP Grating

Continuous glass roving is pulled through a resin bath and die, producing bearing bars with unidirectional strength and high stiffness.

Pultrusion process

Continuous glass roving and mat are impregnated and pulled through a heated die to a precise, repeatable bar cross-section — consistent lengthwise properties every metre.

≈ 70% glass content

Unidirectional bearing bars carry load along their length; roughly 70% glass by weight gives high longitudinal stiffness and strength.

2× stiffness of molded

For the same depth, pultruded bars are roughly twice as stiff and span up to ≈ 3 m — ideal for long platforms and heavy loads.

Bearing-Bar Profile Catalog

Section properties per individual bar (nominal cross-section)

Ix / Zx about the strong (bending) axis; Iy / Zy about the weak axis. Weight per linear metre of bar. Values computed from nominal cross-sections (web/flange ≈ 3 mm) at ≈ 1.85 g/cm³.

ProfileTypeHeight (mm)Width (mm)Weight (kg/m)Area (cm²)Ix (cm⁴)Zx (cm³)Iy (cm⁴)Zy (cm³)
I-4010I-bar40100.301.623.041.520.060.12
I-5010I-bar50100.361.925.452.180.060.12
I-6010I-bar60100.412.228.812.940.060.12
I-4015I-bar40150.361.924.072.030.180.24
I-6015I-bar60150.472.5211.253.750.180.24
T-3320T-bar33200.502.682.831.400.380.38
T-5020T-bar50200.683.709.143.120.410.41
T-6020T-bar60200.804.3015.254.420.430.43

Dimensional check: Zx = Ix / (h/2) holds for every row (e.g. I-6015: 11.25 cm⁴ ÷ 3.0 cm = 3.75 cm³). For design, use certified EI/section data for the exact resin and glass loading; pultruded values are typical and should be confirmed per ASTM D7290 characteristic method.

Assembled Grating Configurations

Standard mesh weights, open area and spans

Bearing bars run across the clear span. Weight includes bars + tie bars; spans are indicative at L/200 for pedestrian live load.

ConfigurationBearing BarBar Centers (mm)Tie BarThickness (mm)Weight (kg/m²)Open AreaMax Span @ L/200 (mm)Max Uniform Load @ 2 m span (kN/m²)
1" × 4" mesh (25 mm bar centers)I-401025Ø6 cross rod @ 100 mm4016.5≈ 55%≈ 1300≈ 3.5
1.5" × 4" mesh (38 mm bar centers)I-401038Ø6 cross rod @ 100 mm4011.5≈ 65%≈ 1500≈ 2.8
2" × 4" mesh (50 mm bar centers)I-401050Ø6 cross rod @ 100 mm409.0≈ 72%≈ 1600≈ 2.2
1.5" × 4" mesh (38 mm bar centers)I-601538Ø8 cross rod @ 100 mm6015.0≈ 62%≈ 2200≈ 7.0
2" × 4" mesh (50 mm bar centers)T-502050Ø8 cross rod @ 100 mm5013.0≈ 70%≈ 2000≈ 6.0
2" × 4" mesh (50 mm bar centers)T-602050Ø8 cross rod @ 100 mm6016.0≈ 70%≈ 2500≈ 9.0

Spans and loads are indicative and consistent with industry pultruded load-table practice; confirm against certified charts for your configuration. Source: Industry pultruded-grating technical brochures (manufacturer data); ZeAllgrate (ACMA) design guidelines.

Physical & Mechanical Properties (Pultruded)

Typical unidirectional laminate values

Longitudinal = along pultrusion / bearing bars; transverse values are significantly lower and are not a design basis.

PropertyTest MethodTypical Value
DensityASTM D7921.7 – 1.9 g/cm³
Glass contentIgnition loss70% ± 5% by weight
Tensile strength, longitudinalASTM D638≈ 300 – 400 MPa (typical)
Flexural strength, longitudinalASTM D790≈ 350 – 450 MPa (typical)
Flexural modulus, longitudinalASTM D790≈ 20,000 – 25,000 MPa (typical)
Compressive strength, longitudinalASTM D695≈ 250 – 300 MPa (typical)
Water absorption (24 h)ASTM D570< 0.2%
Barcol hardnessASTM D2583> 45
CTE, longitudinalASTM D696≈ 5 × 10⁻⁶ /°C
CTE, transverseASTM D696≈ 25 × 10⁻⁶ /°C

Pultruded coupon values are typically ~300–400 MPa tensile and ~350–450 MPa flexural longitudinal — far above molded grating due to ~70% unidirectional glass. Source: Industry pultruded-grating technical brochures (manufacturer data); ZeAllgrate (ACMA) design guidelines.

Tie Bar & Cross-Rod Options

Lateral connection between bearing bars

Tie TypeSizeTop-Surface FinishMaterial / Note
Round cross rod (fiberglass core)Ø6 mm / Ø8 mmFlushed or below top surfaceStandard tie for I-bar gratings; pultruded with resin over-wrap
Round cross rod (stainless steel)Ø6 mm / Ø8 mmFull depth / flushHigher lateral rigidity; specify SS304/SS316 by environment
T-tie barMatching bar depthFlush-topIntegral look; used with T-bar decks for long spans
Flush-top tie barMatching profileTop surface flatSmooth walking surface; ADA-friendly where required
Surface Options & Resin Systems

Grit-top (standard)

Embedded silica grit on the bearing-bar top surface — standard for pultruded grating in wet/chemical service.

Smooth / covered

Smooth natural finish for light pedestrian use; covered (integral) panels available for drip-free decks.

ZeAll ISO (isophthalic, ISOFR)General corrosion grade, self-extinguishing, E84 ≤ 25.
ZeAll VE (vinyl ester, VEFR)Harsh chemical resistance, self-extinguishing; preferred for offshore / process.
ZeAll FR (fire-retardant)Low-flame / low-smoke pultruded formulations with marine (USCG/ABS) options.
Span & Load Reference

Indicative maximum clear spans at deflection limits

Pedestrian live load basis. Lower deflection limit (L/100) gives shorter spans for firmer walking; L/200 is the comfort limit.

ConfigurationMax Clear Span @ L/100 (mm)Max Clear Span @ L/150 (mm)Max Clear Span @ L/200 (mm)
I-4010,1.5" mesh≈ 1900≈ 1600≈ 1400
I-6015,1.5" mesh≈ 2800≈ 2400≈ 2100
T-5020,2" mesh≈ 2600≈ 2200≈ 1900
T-6020,2" mesh≈ 3200≈ 2700≈ 2400

Indicative only. Final design must use certified load/span charts; apply appropriate safety factor (pultruded typically 2:1 F.S. per manufacturer practice). Source: Industry pultruded-grating technical brochures (manufacturer data); ZeAllgrate (ACMA) design guidelines.

Data Sources

  • Industry pultruded-grating technical brochures (manufacturer data) — profiles, mesh configurations and load/span practice.
  • ZeAllgrate (ACMA) Guidelines for the Engineer / Designer — deflection limits, ASTM D7290 characteristic values.
  • Industry molded-grating technical catalogs (manufacturer data) — resin and fire system cross-reference.

Section properties above are computed from nominal cross-sections and are intended for specification-level sizing. ZeAllgrate supplies certified section data and load test reports for each resin and configuration. Contact sales@izeall.com.

Combining Profiles with Grating

Pultruded grating is usually supplied as part of a wider framing package: pultruded I-beams and channels support the panels, angles and flats form borders and stiffeners, and tubes carry handrail posts. Ordering the grating and its framing together from one supplier removes the interface risk — spans, bearing details and clip patterns are coordinated on one drawing set, and the laminate, resin and hardware choices stay consistent across the whole access system.

Mesh, Open Area and Drainage

Pultruded panels are produced in the standard mesh openings — 38 × 38 mm, 25 × 100 mm, and variants — and the open area determines drainage and debris behaviour: larger openings drain faster and carry less wind load on open decks, smaller openings stop tools and feet. For walkways above process equipment, check the mesh against the smallest object the deck must retain; for splash decks, confirm the open area drains the spill volume quickly.

Tolerance and Site Acceptance

  • Panel width, length and flatness verified on arrival against the order tolerance (± 3 mm typical length).
  • Grit-top surface checked for even aggregate coverage; edge chips rejected before installation.
  • Batch marking and certificates matched to the delivery; load test report for the ordered span requested at order stage.
  • Bearing bars oriented along the span at installation; clips placed per the clip schedule.
Certified & Verified

Approved by Industry Bodies, Tested to International Standards

Every ZeAllgrate shipment is backed by documented quality systems, marine approvals and independent third-party verification.

Q

ISO 9001:2015

Certified quality management system — since 2004.

⚓

DNV & ABS Marine

Marine-grade grating for offshore platforms and vessel decks.

✔

SGS & Intertek

Independent third-party inspection and load testing on request.

🛡

OSHA 1910.23

Handrail systems load-tested to US federal requirements.

Material certificates, COA, ASTM test reports and compliance documentation supplied with every order. View certifications →

Need Long-Span Pultruded Grating Sizing?

Tell us your span, live load and deflection limit — we return the exact profile, mesh and clip schedule with certified data within 24 hours.