GRP Grating Color Options & Custom RAL
Quick answer: ZeAllgrate stocks light gray, dark gray, safety yellow, green, red and black GRP grating; custom RAL colors are available from 500 m2. Darker colors resist UV chalk best; bright yellow and red fade faster and should use the UV-stabilized outdoor grade.
Standard GRP grating colors
ZeAllgrate stocks five standard colors, molded into the resin so they cannot peel or wear off. Custom RAL colors are available from 500 m² per color, typically adding 7–10% to the panel price and 7–10 days to lead time.
| Color | Typical RAL | Best for | UV resistance |
|---|---|---|---|
| Light gray | RAL 7035 | Public walkways, municipal, food & beverage | Good |
| Dark gray | RAL 7016 | Industrial platforms, machinery decks | Good |
| Safety yellow | RAL 1023 | Hazard zones, stair nosing, trench edges | Moderate — fades faster in direct sun |
| Safety green | RAL 6024 | Chemical plants, designated walk routes | Good |
| Safety red | RAL 3020 | Emergency routes, fire zones, hazard marking | Moderate |
| Black | RAL 9005 | Grit-top aggregate, coastal / marine decks | Excellent — hides UV chalk best |
Color, resin and UV — what to know
Color is pigmented into the resin, so it does not peel. However, lighter and brighter colors (especially yellow and red) show UV chalk and fade faster than dark gray or black. On outdoor UV-exposed decks, specify the UV-stabilized grade with paraffin surface veil and titanium-dioxide inhibitor; after 5000 hours of QUV-A exposure, color shift stays below ΔE 3. Darker colors also run slightly hotter in direct sun, so on very large outdoor surfaces consider light gray to minimize thermal expansion.
Color-coding best practice
- Yellow for edge warnings, openings, stair nosing and hazard zones.
- Green or blue for designated pedestrian walk routes on multi-use plant decks.
- Red for fire equipment access and emergency egress paths.
- Light gray for general public-facing areas to stay visually clean.
Need a custom RAL match for your project? Send us the RAL number and quantity — we confirm minimum order and price within 24 hours.
Can GRP grating be painted a different color on site?
It is possible to apply a two-part polyurethane gel-coat to cured GRP, but factory-molded color is far more durable and consistent. On-site painting is only recommended for touch-ups or small custom accents, not for whole decks.
Does yellow GRP grating fade in the sun?
Bright safety yellow will chalk and fade faster than gray or black under continuous UV. Specify the UV-stabilized outdoor grade; with that, ΔE color shift stays under 3 after 5000 hours QUV-A, and the panel remains structurally sound for decades.
Need a Quote on GRP / FRP Grating?
Send your chemicals, span and loads — our engineers will recommend the right thickness and resin within one business day.