ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries
Material Properties · 2026-11-17

GRP Grating Weight Per Square Meter

Quick answer: Molded GRP grating weighs 9.5-19 kg/m2 (25-50 mm thick, 38x38 mm mesh); pultruded I-bar grating weighs 22-28 kg/m2. That is roughly one-third the weight of equivalent steel grating (32-65 kg/m2).

How much does GRP grating weigh per square meter?

GRP (glass-reinforced plastic / fiberglass) grating weighs far less than steel — typically 9–20 kg/m² for molded panels and 18–30 kg/m² for pultruded I-bar panels, depending on thickness, mesh pitch and resin system. The table below gives typical values for ZeAllgrate molded and pultruded panels with standard 38×38 mm mesh and isophthalic resin.

TypeThicknessMeshWeight kg/m²Equivalent steel grating
Molded GRP25 mm38×38 mm≈ 9.5 kg/m²≈ 32 kg/m²
Molded GRP30 mm38×38 mm≈ 11.5 kg/m²≈ 38 kg/m²
Molded GRP38 mm38×38 mm≈ 14.5 kg/m²≈ 45 kg/m²
Molded GRP50 mm38×38 mm≈ 19.0 kg/m²≈ 58 kg/m²
Pultruded I-bar50 mm I-bar40×40 mm≈ 22 kg/m²≈ 48 kg/m²
Pultruded I-bar75 mm I-bar50×50 mm≈ 28 kg/m²≈ 65 kg/m²

Why weight matters for your project

A 1.22 × 3.66 m standard molded panel (≈ 4.47 m²) weighs only 42–85 kg depending on thickness — two workers can carry it without a clamp truck. The same panel in galvanized steel would weigh 140–260 kg, requiring mechanical lifting. This weight advantage cuts structural steel support sizes by 15–25% on long-span roofs and mezzanines, reduces shipping and installation labor, and makes FRP the practical choice for retrofits on existing structures that cannot carry extra dead load.

What changes the weight?

  • Thickness — the dominant factor; weight rises roughly linearly with panel depth.
  • Mesh pitch — mini-mesh 19×19 mm is denser and ~10–15% heavier than 38×38 mm open mesh.
  • Resin system — vinylester is ~5% denser than isophthalic; phenolic slightly heavier again.
  • Surface finish — grit-top adds a thin aggregate layer; covered/solid-top panels add ~2 kg/m².

For an exact weight calculation for your project, send us your thickness, mesh and resin grade — we return a stamped panel weight per m² and per standard panel within 24 hours.

How much does 38 mm molded GRP grating weigh?

Approximately 14.5 kg/m² for standard 38×38 mm mesh isophthalic resin. A full 1.22 × 3.66 m panel weighs about 65 kg. Vinylester grade is ~5% heavier; mini-mesh 19×19 mm adds ~12%.

Is GRP grating lighter than aluminum?

Yes. A 38 mm molded GRP panel at ~14.5 kg/m² is roughly half the weight of an equivalent aluminum extruded grating deck, and about one-third the weight of galvanized steel.

Need a Quote on GRP / FRP Grating?

Send your chemicals, span and loads — our engineers will recommend the right thickness and resin within one business day.