Standards & Compliance

ASTM, ISO 14122, OSHA 1910.23, ADA, NEMA and FM — clauses and scope

Test Methods

ASTM Material Test Methods

These are the standard mechanical and physical tests a compliant FRP material data sheet references.

StandardWhat It MeasuresTypical Use
ASTM D638Tensile properties (strength, modulus)Bearing-bar tensile data sheet
ASTM D790Flexural strength & modulusBeam stiffness, load/span design
ASTM D695Compressive propertiesEnd-bearing, crushing at supports
ASTM D792Density / specific gravityMass verification (kg/m²)
ASTM D570Water absorptionMoisture uptake, long-term exposure
ASTM D2583Barcol indentation hardnessSurface cure / quality check
ASTM E84Surface burning (flame spread & smoke)Fire class A/B/C
Safety & Access

Platform, Access & Accessibility Codes

StandardScope & Key ClausesApplies To
ISO 14122 (parts 1–4)Permanent access to machinery. Part 3: stairs, stepladders and guard-rails; defines walkway width, pitch and guard systemsEuropean/ international fixed platforms
OSHA 29 CFR 1910.23Walking-working surfaces: guarding floor/wall openings, standard railings, toe boards and cover requirementsUS general industry platforms
ADA (Americans with Disabilities Act)Accessibility: accessible route surfaces, slip resistance (COF) and level walking surfacesPublic/accessible US facilities
NEMAElectrical/enclosure and fiberglass material standards; non-conductive applicationElectrical rooms, substations
FM Approval (fmGlobal)Insurance-driven approval of grating/construction for specific fire/hazard ratingsOffshore, high-hazard, insured sites

Related regional references: EN ISO 14122 (EU), AS 1657 (Australia), BS 4592 (UK). Always confirm the edition your project references.

Certification

What to Ask a Supplier for

Material Certificate

Glass content, resin type, panel dimensions, thickness, batch number — traceable to production records.

Load Test Report

Actual test panels, span, UDL/concentrated load and deflection — not extrapolated marketing data.

Fire Test Report

ASTM E84 FSI/SDI values, lab identity and product match for the grade shipped.

Standards Map at a Glance

AreaKey StandardsWhat ZeAllgrate Provides
Material testingASTM D790 (flexural), D2584 (burn-off), D2583 (hardness), C581 (chemical)Test reports for the exact grade
Fire performanceASTM E84 (flame spread / smoke)Class A/B/C report; confirm grade and thickness
Walking-working surfacesOSHA 29 CFR 1910.23 / 1910.28Load-tested handrail; load tables for grating
Fixed laddersOSHA 1910.23 / ISO 14122-4Rung spacing, load and cage systems
Access / platformsISO 14122-3Handrail, stairs and platform dimensions

What to Ask a Supplier

  • The test report for the exact resin and construction you are ordering — not a generic brochure value.
  • The load table basis (working vs ultimate) so the safety factor is not double-applied.
  • The E84 class for the grade and thickness, where fire rating is required.
  • Batch certificates matching the delivered panels for traceability.
  • The test report for the exact resin and construction you are ordering — not a generic brochure value.
  • The load table basis (working vs ultimate) so the safety factor is not double-applied.
  • The E84 class for the grade and thickness, where fire rating is required.
  • Batch certificates matching the delivered panels for traceability.

Need a Compliance Package?

ZeAllgrate supplies certificates of conformity, load reports and E84 evidence — ask for your project file.

Source: ZeAllgrate (Fiberglass Grating Manufacturers Council / ACMA) design guidelines; ASTM International; ISO 14122; OSHA 29 CFR 1910. Indicative data for specification guidance only — final design verified by ZeAllgrate engineering against certified load/span charts.