ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

FRP Grating Load & Span Calculator

Free FRP grating load and span calculator: select mesh, thickness and resin to find the maximum allowable span for pedestrian, light vehicle and forklift loads — molded and pultruded.

Calculator

How to Use This Calculator

This FRP grating load and span calculator helps you quickly size a fiberglass reinforced plastic (FRP / GRP) grating panel for your project without opening a full engineering catalog. Follow three simple steps: first, choose whether you need molded FRP grating (bidirectional, square mesh) or pultruded FRP grating (unidirectional I-bar / T-bar, long spans). Second, identify your expected live load: pedestrian walkway (about 5 kN/m²), light vehicle / forklift traffic (10 kN/m²), or heavy forklift / truck loading (25–50 kN/m²). Third, look up the maximum allowable clear span in the tables below for your chosen thickness, mesh and resin.

All span values are the maximum clear distance between supports measured in metres. If your support spacing is larger than the value in the table, either move the supports closer together, select a thicker profile, or upgrade to a pultruded system. The weight column (kg/m² for molded, kg/m for pultruded) helps you estimate dead load, shipping cost and supporting steelwork. For the full imperial charts and resin-specific data, see our dedicated GRP grating load & span tables.

Step 1 — Pick Type

Molded for bidirectional floors, platforms and trenches. Pultruded for long unsupported walkways, bridges and trench covers.

Step 2 — Pick Load

Pedestrian 5 kN/m², light vehicle 10 kN/m², forklift 25 kN/m² (molded) or 50 kN/m² (pultruded).

Step 3 — Read Span

Match thickness × mesh × resin to the load column. Never exceed the tabulated clear span without engineering approval.

Molded FRP

Molded FRP Grating Load & Span Table

Molded FRP (fiberglass reinforced polyester) grating is hand-laid and cured in a square mesh, giving it equal strength in both directions. The table below lists typical maximum clear spans for ZeAllgrate molded panels under three common uniform live loads. Iso = isophthalic polyester resin, VE = vinyl ester, Phenolic = fire-retardant phenolic resin.

ThicknessMeshResinPedestrian (5 kN/m²) Max SpanLight Vehicle (10 kN/m²) Max SpanForklift (25 kN/m²) Max SpanWeight kg/m²
25 mm38×38Iso1.0 m0.7 m—12.5
30 mm38×38Iso1.2 m0.9 m0.6 m14.5
38 mm38×38Iso1.5 m1.1 m0.8 m18.6
38 mm19×19Iso1.4 m1.0 m0.7 m22.5
50 mm38×38Iso1.9 m1.4 m1.0 m24.0
38 mm38×38VE1.5 m1.1 m0.8 m19.8
38 mm38×38Phenolic1.4 m1.0 m0.7 m20.0

Typical clear spans at 20°C ambient, static uniform load. — = not recommended for that load. Source: ZeAllgrate molded grating engineering data.

Pultruded FRP

Pultruded FRP Grating Load & Span Table

Pultruded FRP grating is pulled through a die as continuous unidirectional fiberglass rovings, producing I-bar, T-bar and rectangular bar profiles that span much longer than molded panels. Bearing bars must be oriented across the support direction. The table below lists typical maximum clear spans per metre of bar weight.

ProfileDepthMeshPedestrian (5 kN/m²) Max SpanVehicle (10 kN/m²) Max SpanForklift (50 kN/m²) Max SpanWeight kg/m
I-bar50 mm50×502.5 m1.8 m1.0 m3.5
I-bar75 mm50×503.5 m2.5 m1.5 m5.5
I-bar100 mm50×504.5 m3.2 m2.0 m7.5
T-bar50 mm50×502.2 m1.6 m0.9 m3.0

Bearing bars spanning between supports. Cross rods tie bars together but carry negligible bending. Source: ZeAll pultruded grating load tables.

Design Notes

Safety Factors & Design Notes

The span values above already incorporate a working stress design approach. However, FRP is viscoelastic and its stiffness and strength change with temperature, resin system and glass content. Before you finalise a layout, keep the following engineering rules in mind.

Deflection Limit

Pedestrian walkways: maximum deflection limited to span / 125 under the design live load. Vehicle and forklift areas: tighter limit of span / 200 to avoid user discomfort and vibration. Do not allow deflection to exceed the tabulated value at any point.

Safety Factor

A minimum safety factor of 1.5 on ultimate load is applied to all working values above. For impact, dynamic or fatigue loading (forklift traffic, crane runways, machinery), apply an additional 0.5 reduction — i.e. use half the tabulated span.

Material Variables

Actual load rating depends on resin type (iso / vinyl ester / phenolic), glass fibre content, bar cross-section and ambient temperature. Vinyl ester improves chemical resistance; phenolic improves fire performance but slightly reduces stiffness.

For critical applications — offshore platforms, walkways over hazardous chemicals, truck loading areas, or spans outside the tables above — request a formal engineering calculation from ZeAllgrate. Send your layout drawings, live loads and temperature range to our engineering team and we will return a stamped recommendation within 24–48 hours.

Reading the Tables

How to Read This Table

Each column answers a different design question. Read left to right to narrow down the right panel for your project.

Thickness / Depth. For molded grating this is the overall panel thickness in millimetres (25,30,38 or 50 mm). For pultruded grating this is the bearing-bar depth. Deeper profiles deflect less and span further, but weigh more and cost more.

Mesh. Molded mesh opening in millimetres. 38×38 mm is the standard anti-slip walkway opening; 19×19 mm mini-mesh is used where small objects, tools or shoes must not fall through, and where nosing slip resistance is critical. Pultruded mesh is the centre-to-centre bar spacing.

Resin. Isophthalic (Iso) polyester is the general-purpose corrosion grade for water, wastewater and mild chemicals. Vinyl ester (VE) upgrades resistance to strong acids, alkalis and solvents. Phenolic is the fire-retardant grade for offshore, tunnel and enclosed-space applications where smoke and toxic gas must be minimised.

Max Span columns. Find the column that matches your design live load, then read across to your chosen thickness / mesh / resin row. The number shown is the maximum clear distance between steel supports in metres. If your actual support spacing is equal to or smaller than this number, the panel is acceptable. If it is larger, upgrade the thickness, move the supports, or switch to pultruded.

Weight. Molded weight is per square metre of panel; pultruded weight is per metre of bearing bar. Use these numbers to estimate dead load on supporting steel, crane lifting loads and shipping weight. Remember that grating self-weight deflection is additional to live load deflection.

Not sure which row fits your project? Compare molded vs pultruded in our GRP vs FRP guide, or browse the full FRP grating range and pultruded grating range for product detail.

FAQ

Frequently Asked Questions

What is the maximum span for 38mm FRP grating?

For pedestrian load (5 kN/m²), 38 mm molded FRP grating spans up to 1.5 m between supports. For light vehicle load (10 kN/m²), the maximum span drops to 1.1 m. For forklift traffic (25 kN/m²), the maximum clear span is 0.8 m. If your support spacing is larger, upgrade to 50 mm molded grating or switch to a 50 mm pultruded I-bar, which spans 2.5 m under pedestrian load.

How do I calculate the load rating of FRP grating?

Use the span tables above: select your thickness, mesh and resin, then find the maximum allowable clear span for your design live load (pedestrian 5 kN/m², light vehicle 10 kN/m², forklift 25–50 kN/m²). The table values already include a 1.5 safety factor and deflection limits. For custom calculations — irregular panels, concentrated wheel loads, high-temperature environments or non-standard resin — send your project drawings and loads to sales@izeall.com and our engineers will return a certified load rating.

What's the difference between molded and pultruded span?

Pultruded I-bar grating spans much longer — up to 4.5 m for a 100 mm deep profile under pedestrian load — because it is unidirectional, with continuous rovings running along the bearing bars. Molded grating is bidirectional (equal strength in both directions) but its continuous strand mat is less efficient in bending, so spans top out around 1.9 m even at 50 mm thickness. Choose molded where load acts in both directions or where custom panel sizes matter; choose pultruded for long walkways, trench covers and bridge decks.

Need a Custom Calculation for Your Project?

Send your span, load, resin and temperature requirements — our engineers return a stamped FRP grating load & span recommendation within 24 hours, free of charge.