FRP Grating Panels — Covered, Phenolic & Iso Resin Fiberglass

Fiberglass Grating Panels — Molded & Pultruded
Fiberglass grating panels — also called FRP panels, fibreglass grating or GFRP panels — are open-mesh sheets of glass fibre embedded in a corrosion-resistant resin. ZeAllgrate manufactures them in two engineered formats for industrial flooring, access and drainage.
- Molded panels: bi-directional strength, equal load both directions
- Pultruded panels: I-bar / T-bar / square bar for long spans and heavy loads
- Standard sheet 1220 × 3660 mm; thickness 25 / 30 / 38 / 40 / 50 mm
- Resins: isophthalic, vinyl ester, phenolic, fire-retardant, UV-stabilized
- Non-conductive, spark-resistant, zero-maintenance, 20+ year service life
Molded Fiberglass Grating Panel Sizes
Standard molded panel range — the same configurations our engineers specify for walkways, platforms and trench covers worldwide.
| Parameter | Standard Range |
|---|---|
| Panel size | 1220 × 3660 mm (4′ × 12′) |
| Panel thickness | 25 / 30 / 38 / 40 / 50 mm |
| Mesh pitch | 38×38 / 40×40 / 50×50 mm |
| Mini / micro mesh | 12 / 15 / 20 mm (heel-friendly, toe-passing) |
| Surface | Grit-top anti-slip, concave, convex or smooth |
| Formats | Molded (bi-directional) & pultruded (long-span) |
Full dimension and unit-weight data are in the specification library →.
Resin Systems for Every Environment
We supply three specialty FRP grating panels: covered FRP grating (solid-top, spill-containment), phenolic FRP grating (low-smoke, fire-rated for offshore), and iso resin FRP grating (isophthalic, chemical-resistant for wastewater). Corrosion resistance starts with the resin. Each fiberglass panel system is matched to your media, concentration and service temperature.
| Resin System | Best For | Service Temperature |
|---|---|---|
| Isophthalic (ISO) polyester | General chemical exposure, water/wastewater | 60–70 °C |
| Vinyl ester | Acids, alkalis, solvents | 80–90 °C |
| Phenolic | Fire-critical, low smoke | 120–150 °C |
| Fire-retardant | Code-required flame ratings | ASTM E84 Class B |
| UV-stabilized | Outdoor & solar exposure | UV-stabilized system |
Resin selection is confirmed per application against our certified chemical resistance data →.
Where Fiberglass Panels Are Used
Molded and pultruded fiberglass grating panels replace steel and aluminium where rust, weight and conductivity are a problem.
Walkways
Grit-top anti-slip panels for plant walkways, catwalks and access routes.
Platforms
Heavy-duty panels for processing platforms and raised working floors.
Trench Covers
Load-classed panels for drainage trenches and basin covers.
See the full list of industries served →.
Fiberglass Panels vs Steel vs Aluminium
Why specifiers switch industrial flooring to fiberglass reinforced plastic panels.
| Property | FRP / GRP Panel | Galvanized Steel | Aluminium |
|---|---|---|---|
| Density (approx.) | 1.9 g/cm³ | 7.8 g/cm³ | 2.7 g/cm³ |
| Corrosion resistance | Excellent — non-corrosive | Rusts; zinc coating degrades | Oxidises; pitting in chlorides |
| Electrical conductivity | Non-conductive | Conductive | Conductive |
| Maintenance | Zero, 20+ year service | Re-painting / re-galvanizing | Periodic cleaning |
Standard Panel Sizes Datasheet
Download the full molded and pultruded panel size range for your specification.
Frequently Asked Questions
Standard panels are 1220 × 3660 mm (4′ × 12′), in thicknesses of 25 / 30 / 38 / 40 / 50 mm, with mesh pitches of 38×38,40×40 and 50×50 mm. We also supply mini-mesh panels in 12,15 and 20 mm, and cut panels to your exact footprint.
Molded panels give bi-directional strength with equal load in both directions for platforms, walkways and trench covers. Pultruded panels use I-bar, T-bar and square bar profiles for longer spans and heavier loads.
Isophthalic (ISO) polyester for general chemical exposure, vinyl ester for strong acids, alkalis and solvents, and phenolic for fire-critical low-smoke service. Add fire-retardant (ASTM E84 Class B) and UV-stabilized options for outdoor and code-required service.
Yes — UV-stabilized resin systems are formulated for outdoor and solar exposure, and the panels are non-corrosive to salt water and marine spray, with a 20+ year service life in corrosive service.
Yes. Cut with a carbide or diamond-tipped circular saw, deburr and seal exposed cut edges with resin to prevent moisture ingress. We also factory-cut panels to your drawing.
Covered FRP grating has a solid top sheet bonded over the open mesh. It prevents tools and objects from falling through and contains liquid spills, but reduces drainage — choose standard open mesh where drainage is required.
Specify phenolic for enclosed or confined spaces where fire smoke toxicity is a concern: offshore oil & gas modules, ship interiors, railway and metro stations, tunnels, and battery rooms. It has ASTM E84 Class B fire rating.
Iso resin (isophthalic polyester) is the standard resin for general industrial and wastewater applications — it offers good corrosion resistance at the most competitive price. Upgrade to vinyl ester for strong acids/alkalis, or phenolic for fire-critical areas.
Related Grating Systems
GRP Grating
View →Glass reinforced plastic grating panels, GRP grate and GFRP grating from a certified GRP grating factory.
FRP Grating
View →Molded & pultruded fiberglass reinforced plastic grating for walkways, platforms and drainage.
Fiberglass Grating
View →Fiberglass grating panels, fiberglass grating and GFRP grating for industrial flooring.
Pultruded FRP Grating
View →Long-span pultruded fiberglass bar grating in I-bar, T-bar and square bar profiles.
GRP Grating Standard Sizes
View →Standard panel dimensions, thicknesses and mesh openings for ordering.
Molded FRP Grating
View →Bi-directional molded fiberglass grating panels with grit-top anti-slip surfaces.
Explore FRP Grating Types
Choose the right fiberglass grating, GRP grating and composite grating for your project — molded, pultruded, grille and clip systems.
FRP Grating
View →Molded & pultruded FRP grating panels, FRP grate and composite grating for walkways, platforms and trench covers.
GRP Grating
View →Glass reinforced plastic grating panels, GRP grate and GFRP grating from a certified GRP grating factory.
Fiberglass Grating
View →Fiberglass grating panels, fiberglass grate and fibreglass grating for industrial flooring and walkways.
FRP Grille
View →Fiberglass grille, tree grate, tree pit grating and architectural FRP grate.
Pultruded FRP Grating
View →Pultruded fiberglass grating, pultruded GRP grating and FRP pultruded bar grating for long spans.
Grating Clips & Clamps
View →FRP grating clips, clamps and fasteners in SS304/SS316 and galvanized steel.
Specifying Fiberglass Grating Panels?
Send us your panel size, thickness and environment — we’ll confirm availability and pricing within 24 hours.
Resin Systems for FRP Grating Panels
Choose the resin based on your chemical environment, fire rating requirement and budget.
| Resin | Best Environment | Corrosion | Fire Rating | Relative Cost |
|---|---|---|---|---|
| Isophthalic (iso) | General industrial, wastewater, mild chemicals | Good | ASTM E84 Class B/C | Base |
| Vinyl ester (VE) | Acid & alkali, offshore, pulp & paper | Excellent | ASTM E84 Class B | +30–50% |
| Phenolic | Offshore, enclosed platforms, transit tunnels | Very good | ASTM E84 Class B (low smoke) | +80–120% |
| Polyester (general) | Dry indoor, architectural, UV outdoor | Fair | Self-extinguishing | -10% |
Covered, Phenolic & Iso Resin Specialty Panels
Beyond standard molded and pultruded panels, we supply three specialty FRP grating panel types:
| Panel Type | Top Surface | Key Benefit | Typical Use |
|---|---|---|---|
| Covered FRP grating | Solid flat top | Retains dropped objects, contains spills | Walkways over equipment, battery rooms |
| Phenolic FRP grating | Gritted or concave | Low smoke, low toxicity, fire-rated | Offshore modules, train stations, tunnels |
| Iso resin FRP grating | Gritted / concave | Balanced corrosion resistance at base cost | Wastewater, chemical plants, general industry |
Fire Rating & Compliance
Our phenolic FRP grating panels achieve ASTM E84 Class B flame spread index ≤ 25 and smoke developed index ≤ 450, making them suitable for offshore modules, marine interiors, railway stations, tunnels and enclosed platforms where low smoke and low toxic fume emission is critical. Iso resin and vinyl ester panels achieve Class B/C. All panels meet OSHA 1910.23 walking-working surface requirements.