ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

Fiberglass Grating (Fibreglass) — Molded & Pultruded Panels

Molded & pultruded fiberglass grating panels — fibreglass grating, fiberglass grate and GFRP grating for industrial flooring, walkways and platforms — by ZeAllgrate.

What is fiberglass grating?

A fiberglass grate (also called fiberglass, FRP or GFRP grating) is a lightweight, corrosion-resistant open-mesh panel of glass fiber in resin — the non-conductive alternative to steel walkways.

Fiberglass grating (also called FRP or GFRP grating) is an industrial flooring panel made from glass-fiber reinforcement — typically 50–65% glass fiber and 30–45% resin (polyester, vinyl ester or phenolic) plus 5–10% additives for UV, fire and color. The resin protects the fibers from chemicals, moisture and UV, while the open mesh drains water and cuts weight. It is 70–80% lighter than steel, non-conductive, non-magnetic and slip-resistant, used for industrial platforms, chemical plants, wastewater, marine/offshore and cooling towers. ZeAllgrate supplies both molded fiberglass grating and pultruded fiberglass grating, cut to size, ISO 9001 certified, exported to 45+ countries.

38 mm
Standard mesh depth
Class A
ASTM E84 flame rating
4 resins
Ortho / ISO / VE / Phenolic
ISO 9001
SGS audited · 45+ countries

Fiberglass grating = FRP = GFRP = GRP — same composite, regional names. North America says "FRP" or "fiberglass grating"; the UK and Commonwealth say "GRP" (Glass Reinforced Plastic); engineering drawings and academic papers say "GFRP" (Glass Fiber Reinforced Polymer). ZeAllgrate supplies all four name variants from one ISO 9001 line.

Fiberglass Grille vs Fiberglass Grating: Same Product, Different Word

In export listings and buyer RFQs, fiberglass grille, FRP grille, or GRP grille are used interchangeably with fiberglass grating. They all refer to the same open-mesh fiberglass reinforced plastic panel on this page. If your drawing or supplier quote says "grille", it means the product covered here.

ZeAllgrate fiberglass grating panels
Product Overview

ZeAllgrate Fiberglass Grating Systems

As a long-established fiberglass grating supplier, ZeAllgrate produces molded and pultruded fiberglass grating — also specified as fibreglass grating, fiberglass grate, GFRP grating or fiberglass reinforced plastic grating — for industrial flooring, walkways and platforms in corrosive service.

  • Molded fiberglass grating: bi-directional strength panels for floors and trench covers
  • Pultruded fiberglass grating: long spans with I-bar, T-bar and square bar profiles
  • Industrial fiberglass flooring grating & fiberglass floor grating panel formats
  • Resin systems: isophthalic, vinyl ester, phenolic, fire-retardant, UV-stabilized
  • Fiberglass mesh grating and mini/micro mesh fine-opening options
  • Non-conductive, corrosion resistant fiberglass grating — 20+ year service life

Also available as grit-top, gritted & covered fiberglass grating →

Terminology

Fiberglass Grating vs FRP vs GFRP — One Product, Three Names

Fiberglass grating, FRP grating and GFRP grating all describe the same composite open-mesh panel: continuous glass fibre reinforcement locked inside a corrosion-resistant polymer resin. The name simply reflects the market and the abbreviation in use.

  • Fiberglass grating / fibreglass grating — the everyday term across North America and the UK, describing glass fibre in resin.
  • FRP grating (Fibre Reinforced Plastic) — the engineered abbreviation used on datasheets, drawings and procurement specs.
  • GFRP grating (Glass Fibre Reinforced Polymer) — increasingly used in European and engineering-standard documents.
  • All three are manufactured on the same ZeAllgrate line and carry identical mechanical, electrical and corrosion properties.

Whichever name your spec uses, the panel we ship is the same ISO 9001-certified product. See our grating terminology glossary →

Composition

What Is Fiberglass Grating Made Of?

The performance of fiberglass grating comes from its two ingredients: the glass fibre reinforcement and the resin matrix. Getting both right is what separates a 20-year panel from a panel that fails early.

  • Glass fibre (60-70% by weight) — E-glass rovings and mat deliver the tensile strength; the higher the glass content, the stiffer and stronger the panel.
  • Resin matrix (30-40%) — isophthalic polyester for general chemical service, vinyl ester for acids and alkalis, phenolic for fire-critical low-smoke service.
  • Surface veil — a corrosion barrier layer that protects the glass from chemical attack and micro-cracking.
  • Optional additives — UV stabilizers for outdoor exposure and flame-retardant fillers for code-required fire ratings.

Glass content and resin are matched per application. Ask for our material property datasheet →

Surface & Finish

Fiberglass Grating Surfaces & Anti-Slip Finishes

The walking surface of fiberglass grating is a specification decision, not an afterthought. ZeAllgrate offers the full range of anti-slip options.

SurfaceDescriptionBest For
Grit-topEmbedded silica/alumina grit for aggressive slip resistanceWet, oily, food and chemical zones
ConcaveCurved profile that drains and improves slip performanceWalkways and platforms under light water
ConvexDomed top surface, gentle on barefoot / light trafficDock and leisure decking
SmoothFlat surface for easy cleaning and tool-free trolley trafficMaintenance access and mechanical rooms

Need colour-matched panels for architectural projects? Custom RAL colours are available on molded and pultruded fiberglass grating.

Standards

Fiberglass Grating Standards & Compliance

Fiberglass grating is specified against internationally recognised load, fire and access standards. ZeAllgrate panels are tested and certified to the relevant codes.

  • Fire — ASTM E84 Class B flame spread (≤ 25), plus ASTM D3841 for glass-fibre reinforced panels.
  • Mechanical — ASTM D790 flexural properties and D638 tensile data on every production batch.
  • Access — working platforms engineered to EN ISO 14122 and OSHA 1910.23 load requirements.
  • Quality — ISO 9001:2015 certified manufacturing, with material and load certificates per shipment.

Full standards & compliance guide →

Lifecycle

Fiberglass Grating Lifecycle & Whole-Life Cost

Fiberglass grating is bought once and forgotten. Across a 20-year industrial service life it typically costs less than galvanized steel, which needs re-coating, re-galvanizing or replacement.

  • Zero maintenance — no painting, no galvanizing, no rust patching.
  • Non-corrosive — immune to chlorides, acids, alkalis and marine salt spray.
  • Non-conductive — dielectric, spark-resistant, safe in electrical and ATEX zones.
  • Lightweight — roughly a quarter of steel density, cutting freight and installation cost.

Model the lifecycle saving against steel for your project — engineering tools →

Grating Types

Molded & Pultruded Fiberglass Grating — Two Engineered Formats

Molded fiberglass grating is the most common walkway panel, while our pultruded fiberglass grating is preferred for long spans. In the UK and Australia, customers search for "fibreglass grating" — the same product, British spelling. Choose the format that matches your span, load and environment. Both are fiberglass reinforced plastic grating built for decades of zero-maintenance service.

M

Molded FRP Grating

Compression-molded, bi-directional strength panels for platforms, walkways and trench covers.

View range →
P

Pultruded FRP Grating

Unidirectional I-bar / T-bar / square bar grating for long spans and heavy loads.

View range →
C

FRP Grating Covers

Trench cover grating, basin covers and screening covers with load class ratings.

View range →
🔩

FRP Grating Clips

SS304/SS316 grating clips, clamps and fasteners for secure installation.

View range →
Applications

Where Fiberglass Grating Is Specified

Industrial fiberglass flooring grating, fiberglass platform grating and fiberglass walkway grating are specified wherever rust, weight or conductivity rule out steel.

Floors, Walkways & Platforms

Wet, Outdoor & Utility

See our applications guide → and the full industry list →.

Properties & Panel Formats

Corrosion-Resistant, Lightweight & Non-Conductive

Every property requirement — from corrosion resistant fiberglass grating to fire retardant fiberglass grating — is a standard configuration, not a special order.

Performance Properties

  • Corrosion resistant fiberglass grating
  • Fire retardant fiberglass grating
  • Lightweight fiberglass grating
  • Non conductive fiberglass grating
  • Anti-slip grit-top fiberglass grating
  • UV-stabilized outdoor fiberglass grating

Panel Formats

  • Fiberglass floor grating panel
  • Fiberglass mesh grating
  • Fiberglass grate / fibreglass grating open-mesh
  • GFRP grating panel
  • Mini-mesh & micro-mesh fiberglass grating
  • Cut to size fiberglass grating
  • Custom fiberglass reinforced plastic grating
Types & Resins

Fiberglass Grating Types & Resin Systems

Select the grating type and resin system matched to your environment — the same methodology our engineers apply to every quotation.

OptionBest ForKey Property
Molded fiberglass gratingFloors, platforms, walkways, trench coversBi-directional strength, 25-50 mm thick
Pultruded fiberglass gratingLong spans, pipe racks, heavy loadsI-bar / T-bar / square bar, high strength-to-weight
Mini mesh fiberglass gratingSmall-part fall-through preventionFine 19.05 × 19.05 mm mesh top
Micro mesh fiberglass gratingPublic access, small openingsSmall opening with anti-slip profile
Fiberglass phenolic gratingFire-critical, low smokePhenolic resin, 120-150 °C
Iso resin fiberglass gratingGeneral chemical exposureIsophthalic polyester, 60-70 °C
Vinyl ester fiberglass gratingAcids, alkalis, solventsSuperior corrosion resistance, 80-90 °C

Resin guidance is confirmed per application against our certified chemical resistance data. Full chemical resistance guide →

Manufacturer Direct

Fiberglass Grating Manufacturer & Supplier

ZeAllgrate is an established fiberglass grating manufacturer and fiberglass grating supplier serving distributors and projects in 45+ countries since 2004. We support custom fiberglass grating, cut to size fiberglass grating, OEM/ODM branding and export packaging, with material certificates and load test reports with every shipment.

  • Factory-direct pricing from our ISO 9001:2015 certified facility
  • Cut to size fiberglass grating and custom panels to your drawing
  • OEM/ODM support with private-label packaging
  • Export packing: wooden crates, fumigation certificates, full documentation
Engineering data

Mechanical Properties: Molded vs Pultruded Fiberglass Grating

Typical values for polyester/vinyl-ester resin systems. Glass fiber volume ratio (FVR) distinguishes the two processes.

PropertyMolded fiberglass gratingPultruded fiberglass grating
Tensile strength60–100 MPa200–350 MPa
Flexural strength (ASTM D790)150–250 MPa350–500 MPa
Modulus of elasticity7–12 GPa20–30 GPa
FVR (fiber volume ratio)25–35%55–70%
38 mm panel live load @ 1 m span3.0–5.0 kN/m²7.5–9.0 kN/m² (I-bar)
Open area30–40%50–70%
Direction of strengthBidirectionalUnidirectional (along bars)

Coefficient of thermal expansion: ~20–25 × 10⁻⁶/°C — ~24% lower than aluminium, ~50% lower than steel, for stable long-run walkways with fewer expansion joints.

Selection guide

Which Fiberglass Grating Spec for Which Application?

Quick spec lookup by use case — thickness, mesh, surface, and resin matched to environment.

ApplicationThicknessMeshSurfaceResin
Light walkway / pedestrian platform25 mm38×38 mmGrittedIsophthalic polyester
Industrial platform / mezzanine38 mm38×38 mmGrittedIsophthalic / vinyl ester
Chemical plant / acid & alkali38–50 mm38×38 mmConcaveVinyl ester
Marine / offshore / jetty deck38–50 mm38×38 mmGritted / coveredVinyl ester
Wastewater treatment plant38 mm38×38 mmConcave / grittedVinyl ester
Fire-critical / offshore tunnel50 mm38×38 mmGrittedPhenolic (Class A)
FAQ

Frequently Asked Questions

What is fiberglass grating?

Fiberglass grating is an open-mesh panel of glass fibre set in a corrosion-resistant resin — also called fibreglass grating (UK spelling), FRP grating, GRP grating, GFRP grating or fiberglass reinforced plastic grating. It is a lightweight, non-conductive, rust-proof alternative to steel and aluminium grating for industrial flooring, walkways and platforms.

Fibreglass or fiberglass — same material?

Yes. 'Fibreglass grating' and 'fiberglass grating' are the identical product — the same glass-fibre reinforced resin — just British versus American spelling. ZeAllgrate supplies both fiberglass grate and fibreglass grating panels from the same ISO 9001 production line.

What is GFRP grating?

GFRP grating (Glass Fibre Reinforced Plastic) is the technical abbreviation for the same material as fiberglass grating and GRP grating. Whether you specify GFRP grating, fibreglass grating or FRP grating, ZeAllgrate molds and pultrudes it to the same panel sizes, mesh pitches and load ratings.

Can you supply cut to size fiberglass grating?

Yes. As a fiberglass grating supplier since 2004, we stock standard panels up to 1220 × 3660 mm and fabricate cut to size fiberglass grating and custom fiberglass floor grating panels to your drawing, with holes, notches and special mesh — plus export packing to 45+ countries.

Related Products

Related Grating Systems

F

FRP Grating

View →

Molded & pultruded fiberglass reinforced plastic grating for walkways, platforms and drainage.

G

GRP Grating

View →

Glass reinforced plastic grating panels, GRP grate and GFRP grating — molded & pultruded.

P

Pultruded FRP Grating

View →

Long-span pultruded fiberglass bar grating in I-bar, T-bar and square bar profiles.

M

Molded FRP Grating

View →

Bi-directional molded fiberglass grating panels with grit-top anti-slip surfaces.

🌱

FRP Grille

View →

Fiberglass grille, tree grate, tree pit grating and architectural FRP grate.

🔩

Grating Clips & Clamps

View →

FRP grating clips, clamps and fasteners in SS304/SS316 and galvanized steel.

Grating Type Guides

Explore FRP Grating Types

Choose the right fiberglass grating, GRP grating and composite grating for your project — molded, pultruded, grille and clip systems.

F

FRP Grating

View →

Molded & pultruded FRP grating panels, FRP grate and composite grating for walkways, platforms and trench covers.

G

GRP Grating

View →

Glass reinforced plastic grating panels, GRP grate and GFRP grating from a certified GRP grating factory.

F

Fiberglass Grating

View →

Fiberglass grating panels, fiberglass grate and fibreglass grating for industrial flooring and walkways.

🌿

FRP Grille

View →

Fiberglass grille, tree grate, tree pit grating and architectural FRP grate.

P

Pultruded FRP Grating

View →

Pultruded fiberglass grating, pultruded GRP grating and FRP pultruded bar grating for long spans.

🔩

Grating Clips & Clamps

View →

FRP grating clips, clamps and fasteners in SS304/SS316 and galvanized steel.

UK spelling

Fibreglass Grating

Fibreglass grating is the UK/Commonwealth spelling of the same fiberglass grating panel used across chemical, water-treatment and marine access. Whether specified as fibreglass, fiberglass or GFRP, ZeAllgrate supplies the molded and pultruded panel in grit-top and concave anti-slip surfaces.

Specify Fiberglass Grating?

Send us your dimensions, load and environment — we'll confirm availability and pricing within 24 hours.

Need a Spec for Your Span & Load?

Send your application, span and chemical environment — our engineers reply with a matched thickness, mesh, resin and clip schedule within one business day. Free samples available for qualified projects.

Request a Quote   Browse Products

More applications

Fiberglass Grating in Specialty Service

Car wash & detailing bays

Chemical-resistant vinyl-ester grating withstands detergents, degreasers and hot water under repeated vehicle traffic. Covered top option keeps suds and runoff contained.

Food & beverage plants

Smooth or gritted surfaces that withstand washdown, steam and mild acids. Non-corrosive to cleaning chemicals; no rust contamination on product lines.

Electrical substations

Non-conductive, non-sparking walkways around switchgear and transformers. Surface resistance ≥10¹² Ω·cm; safe for live maintenance access zones.

Before you ask

Buyer's Quick Checklist

Send these seven items with your RFQ and our engineers will match the exact panel spec within one business day.

1. ApplicationWalkway, platform, chemical trench, marine deck, stair tread, drainage cover?
2. SpanClear unsupported distance between bearers (600 / 800 / 1000 / 1200 mm or other)
3. Thickness25 mm light walkway / 38 mm standard industrial / 50 mm heavy load
4. Mesh opening38×38 mm standard / 25×25 mm chemical / 19×19 mm ADA micromesh
5. SurfaceGritted / concave / covered solid / conductive anti-static / translucent
6. ResinIsophthalic general / vinyl ester acid & alkali / phenolic fire-critical
7. Fixing clipsSS304 dry indoor or SS316 marine/chemical; min 4 per 1220×3660 mm panel