How to Read FRP Grating Load Charts & Span Tables
Quick answer: FRP grating load capacity depends on panel depth (25/38/50 mm), span, and load type (concentrated vs uniform). A 38 mm panel at 915 mm span supports ~167 kgf concentrated or 1,200 kgf/m² uniform. Always verify against certified load charts. For a broader overview of GRP grating types and specifications, see our technical guide.
A load chart is the contract between a grating panel and its supports. Read it correctly and your walkway stays within deflection limits for decades; read it loosely and panels flex, clip and fail early.
Two Load Types You Will See
Uniform load (kN/m²) simulates distributed weight — a crowd of people, a layer of product, an equipment mat. Concentrated load (kN) simulates a single heavy point — a forklift wheel, a machine foot, a dropped load. Both must be checked against the chart for your span.
Deflection: The Real Limit
Specifications typically limit deflection to L/100, L/150 or L/200 of the clear span. Longer spans and lighter panels deflect more. If your project specifies L/200, the allowable load is lower than L/100 on the same panel — always verify the deflection criterion before comparing charts.
Span Direction Matters
Pultruded grating carries load along the bearing bars only — orient bars across the short span. Molded grating carries load in both directions. Reversing a pultruded panel is the single most common specification error on site.
ZeAllgrate provides certified load/span charts for every configuration — send your span, load and deflection requirement and we return the exact panel recommendation.
Reading the Chart: A Worked Example
Take a process walkway with a clear span of 1.2 m and a specified uniform load of 4.0 kN/m² at a deflection limit of L/150. On the ZeAllgrate chart for molded grating, locate the 1.2 m span column, read down until the tabulated allowable uniform load reaches or exceeds 4.0 kN/m², and confirm the panel thickness and resin grade printed in that row. If the same walkway were specified at L/200, the allowable load for the identical panel drops — the chart's second block for the same span carries the L/200 values, and a thicker panel or closer supports may be required. Always read the chart at the deflection limit your specification names, not the one printed largest.
Safety Factors and Allowable Loads
Published chart values are allowable loads, not ultimate capacities. The tests establish ultimate strength, and the published values apply a safety margin consistent with the relevant design code and the service factor for the resin and environment. When combining loads — a uniform crowd load plus a concentrated equipment point — check each load case separately against the chart, then verify the combined effect against the deflection limit. In high-temperature chemical service, de-rate the allowable load in line with the resin manufacturer's elevated-temperature factors; a chart generated at 23 °C does not apply unchanged at 70 °C.
Concentrated Load Cases
Forklift wheels, machine feet and dropped loads are checked as concentrated loads in kN. The governing case is the heaviest single wheel or foot, applied at the worst position — usually mid-span — because that is where deflection is greatest. If the concentrated capacity at your span is marginal, the practical fixes are a deeper panel, a shorter span, or pultruded grating whose aligned bars concentrate stiffness where the wheel runs. Note that many codes require both uniform and concentrated cases to pass independently; a panel that passes the uniform case can still fail the point-load case at mid-span.
Common Chart Errors on Site and in Specs
- Wrong span direction — pultruded capacity is valid only with bearing bars across the span; reversing the panel invalidates the chart value.
- Mixing deflection limits — comparing an L/100 value from one vendor with an L/200 value from another overstates the real capacity.
- Ignoring support conditions — charts assume adequate bearing and clipping at every support; a panel resting unclipped on two beams does not develop the tabulated capacity.
- Using room-temperature values for hot service — always apply the elevated-temperature de-rating factor before comparing against the load requirement.
Deflection Limits at a Glance
| Limit | Typical Use |
|---|---|
| L/200 | Walkway default; general foot traffic |
| L/150 | Heavy maintenance platforms; less strict |
| L/100 | Industrial service where small deflections are acceptable |
| Project-specific | Cleanrooms, vibration-sensitive decks; tighter than L/200 |
Unit Discipline
Span tables are published in kN/m² with metre spans or in psf with feet — pick one system and stay in it. A common error is mixing a psf load with a metre span, which shifts the result by the unit factor and can select the wrong panel. Note whether the table is working load (safety factor included) or ultimate (factor to be applied), and confirm the concentrated column is checked alongside the uniform column — the point load governs on many walkways.
How to Read a Grating Load Chart
A load chart answers one question: at this support span, how much load can this panel carry without exceeding stress or deflection. There are two load types. Uniformly distributed load (UDL) is the whole deck in psf or kg/m². Concentrated load (CL) is a point or wheel load, in kgf, that must not punch through. Check both — a walkway can pass UDL and still fail a 136 kg maintenance-man point load on a short bar pitch.
The deflection limit
Charts are normally published to a deflection limit, commonly span/120 for pedestrian access (ISO 14122 and AS 1657 reference similar limits). A panel that bends more than span/120 feels springy and cracks its surface veil, even if the glass never breaks. If your project specifies span/180, size to the tighter limit.
Indicative UDL Table by Bar Depth and Span
The table converts ZeAllgrate pultruded UDL values to approximate psf, for grit-top panels sized to a deflection limit. These are indicative starting values — confirm the certified load chart for your exact configuration before ordering.
| Clear span | 38 mm bar | 50 mm bar | 60 mm bar |
|---|---|---|---|
| 0.61 m (2 ft) | ~1,180 psf | ~1,560 psf | ~2,050 psf |
| 0.91 m (3 ft) | ~570 psf | ~780 psf | ~1,000 psf |
| 1.22 m (4 ft) | ~350 psf | ~490 psf | ~635 psf |
| 1.52 m (5 ft) | ~225 psf | ~330 psf | ~430 psf |
| 1.83 m (6 ft) | ~155 psf | ~225 psf | ~300 psf |
Read it like this: a 50 mm pultruded panel on 1.22 m centres carries roughly 490 psf UDL to the deflection limit. Standard industrial walkways run 100–150 psf, so 50 mm bar on 1.2 m centres has comfortable margin; a truck or forklift route needs a dedicated wheel-load check, not the UDL row.
Common Industrial Loads to Compare Against
| Application area | Typical UDL demand | Notes |
|---|---|---|
| Pedestrian walkway | 100–150 psf | Standard access; point load ~136 kg |
| Process / equipment platform | 150–300 psf | Tools, drums, occasional stands |
| Maintenance / valve platform | 100–200 psf | Local point loads govern |
| Mezzanine / elevated floor | 200–500 psf | Code-specified; check CL |
| Vehicle / forklift route | Engineer review | Wheel load, not UDL |
A Worked Deflection Example and Fatigue
Take a 50 mm pultruded panel, 1.2 m clear span, 100 psf load. Certified UDL is roughly 490 psf to span/120, so utilisation is about 0.20 — comfortable. If the project tightens the limit to span/180, allowable UDL drops to roughly 0.6–0.7 of the span/120 figure, and the engineer may move from 38 mm to 50 mm bar. A chart rated for static UDL does not automatically cover repeated wheel traffic; plant carts and drum trolleys impose cyclic point loads that fatigue the bar-to-tie connection — these need engineering review, not a lookup. Pair pultruded decks with pultruded support framing so support stiffness is not the weak link.
Common Load-Chart Mistakes
- Using UDL for wheel loads. UDL and CL are separate checks.
- Ignoring the deflection limit. Stress passing is not enough — span/120 usually governs.
- Bar orientation wrong. Pultruded bars must run across the span.
- Forgetting cut-outs. Openings reduce capacity and need edge support.
- De-rating for temperature. Above ~50 °C, stiffness drops; re-size or upgrade resin.
Send support spacing, design UDL and any point/wheel loads; engineering returns a certified size with matching molded or pultruded panel, backed by load test reports.
Open Area, Drainage and the Chart
Load capacity and open area trade off: a larger mesh drains better and weighs less, but the bar width contributing to the structural section drops. In drainage and grate roles, choose the mesh for flow first, then re-check that the load chart at that open area still carries the design load — a 60% open panel and a 40% open panel are not the same structural section even at equal bar depth. Pair drainage decks with matching FRP grating covers where openings need sealing, and confirm the final open-area panel against the certified chart.
Where to Get the Certified Chart for Your Panel
Every ZeAllgrate order is backed by load test reports and material certificates, and published charts cover standard I/T bar configurations (25–60 mm bar depths, 25.4–50.8 mm centres). For custom mesh, special resin or non-standard spans, the chart is re-run for your configuration — contact engineering with support spacing, design UDL and any point/wheel loads. Do not size from a generic online table; use the certified values for the exact panel you will install.
Discuss Your FRP Project
Talk to our engineers about your application — free technical consultation.
Frequently Asked Questions
A 38 mm molded panel at 915 mm span supports ~167 kgf concentrated load or 1,200 kgf/m² uniform load. Capacity varies by depth (25/38/50 mm), mesh, span, and load type.
Maximum clear span depends on depth: 25 mm ~0.9 m, 38 mm ~1.2 m (pedestrian), 50 mm ~1.5 m. Always use L/200 deflection limit and verify against certified load/span charts.
Heavy-duty 50 mm pultruded grating can support forklift traffic at reduced spans. Specify HLC (Heavy Load Capacity) configurations and verify wheel loads against manufacturer data.
Frequently Asked Questions
How do I read an FRP grating load chart?
Find your panel thickness (#25, #38, #50, #75), match your live load (e.g. 5 kN/m2 pedestrian), and read the maximum allowable span under the L/180 deflection limit.
What deflection limit should I use?
Most specifications use L/180 for pedestrian walkways and L/240 for platforms where vibration control matters. Heavy-duty decks or public access areas may use L/360.
What is the maximum span for #38 molded grating?
At 5 kN/m2 (pedestrian load), #38 vinyl ester molded grating spans up to 1.5 m center-to-center. At 10 kN/m2 the allowable span drops to about 1.0 m.
Do I need a safety factor?
Yes. Load charts already include a typical safety factor of 3:1 on ultimate strength. For dynamic loads or heavy point loads, apply an additional 1.5x span reduction.