ISO 9001 Certified · FRP/GRP Grating Manufacturer · Since 2004 · Exporting to 45+ Countries

FRP Resin Selection Wizard

Score five resin systems against your service conditions

Wizard

FRP Resin Selection Wizard

Answer five service questions. Each resin is scored 0–10 per criterion, weighted and summed; the two best-scoring resins are recommended with a cost index. The strictest single requirement (strongest chemical, hottest service, strictest fire code) should normally govern.

1 · Your Service Conditions

Recommendation

Run the wizard to see top resins.

Select your service conditions and press Recommend a Resin — the top two resin systems are scored and ranked.

Reference Table

Resin Systems Compared

Typical, indicative property ranges. Actual grades vary by manufacturer and formulation; confirm against the approved datasheet for the grade quoted.

Resin SystemGlass Transition TgMax Continuous Temp.Chemical ResistanceFire PerformanceTypical ApplicationsCost Index
Orthophthalic Polyester70 – 90 °C≈ 60 – 80 °CGood to moisture / mild acids; limited vs. oxidizers & solventsSelf-extinguishing; typically Class CDry, non-corrosive walkways; general building1.0×
Isophthalic Polyester100 – 120 °C≈ 80 – 100 °CGood acids, alkalis, moisture and saltwater; the cost workhorseClass B with FR formulationStandard plant, wastewater, marine splash, cooling towers1.3×
Vinyl Ester120 – 150 °C≈ 120 °CExcellent strong acids, oxidizers, chlorine bleach & brineClass B (Class A with FR grade)Chemical processing, offshore, pulp & paper1.8×
Fire-Retardant Vinyl Ester110 – 130 °C≈ 110 °CExcellent chemical resistance with halogenated / FR formulationClass A / B ASTM E84Fire-rated chemical areas, offshore modules1.8 – 2.0×
Phenolic> 200 °C≈ 150 – 200 °C+Good acids & solvents; lower vs. strong alkalisInherently Class A, very low smoke & toxicityTunnels, escape routes, offshore accommodation2.5×

Food contact and potable-water service additionally require an approved food-grade / potable-water resin grade (e.g. FDA / WRAS / KTW-compliant). UV service requires a UV-stabilized resin grade.

Need a Confirmed Resin & Datasheet?

List every chemical by name, concentration and temperature — we match the resin and share technical datasheets and test evidence.

Design basis: ZeAllgrate (Fiberglass Grating Manufacturers Council / ACMA) design guidelines; ASTM D790 (flexural properties), ASTM D638 (tensile), ASTM D648 (heat deflection) and ASTM E84 (surface burning). Resin property data based on Ashland / Reichhold technical datasheets. All outputs are INDICATIVE estimates for specification guidance only — they are NOT a substitute for certified load/span charts, approved resin datasheets or professional engineering judgment. Final design must be verified by ZeAllgrate engineering.